Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.451 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.829 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 180.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 287.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 238.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 238.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 180.8 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 287.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 255.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 271.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 238.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 271.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 287.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 180.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 255.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 159.2 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 140.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 90.4 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 159.2 |
LaF3 (mp-905) | <1 0 1> | <1 0 1> | 140.8 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 90.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 255.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 180.8 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 238.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 180.8 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 -1> | 287.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 255.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 238.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 238.7 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 238.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 238.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 180.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 159.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 90.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 140.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 318.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 271.2 |
Ga2O3 (mp-886) | <1 1 -1> | <0 1 1> | 156.4 |
Si (mp-149) | <1 0 0> | <1 0 0> | 238.7 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 156.4 |
Au (mp-81) | <1 0 0> | <0 1 1> | 156.4 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 318.3 |
C (mp-48) | <0 0 1> | <1 1 1> | 190.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 180.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 90.4 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 271.2 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 238.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 271.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 287.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 180.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 -1> | 191.8 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 79.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrGeO3 (mp-17464) | 0.2730 | 0.000 | 3 |
CaSiO3 (mp-17552) | 0.2272 | 0.020 | 3 |
YBO3 (mp-29205) | 0.2854 | 0.000 | 3 |
BaSiO3 (mp-776084) | 0.2125 | 0.000 | 3 |
CaSiO3 (mp-561086) | 0.2408 | 0.020 | 3 |
Na2ZnP2O7 (mp-6491) | 0.5659 | 0.005 | 4 |
YSiNO2 (mp-559123) | 0.4576 | 0.008 | 4 |
Rb2MnV2O7 (mp-19472) | 0.5823 | 0.135 | 4 |
Na2CoP2O7 (mp-24887) | 0.5701 | 0.021 | 4 |
YSiNO2 (mp-559569) | 0.4427 | 0.005 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Si O |
Final Energy/Atom-7.4213 eV |
Corrected Energy-235.2813 eV
-235.2813 eV = -222.6401 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)