Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.553 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.386 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 63588 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 0 0> <0 1 0> 0.011 196.9
Al (mp-134) <1 0 0> <0 1 0> 0.013 196.9
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.017 185.5
C (mp-66) <1 0 0> <1 0 1> 0.020 192.8
YAlO3 (mp-3792) <1 1 1> <0 1 1> 0.022 251.4
GaAs (mp-2534) <1 0 0> <0 1 0> 0.024 196.9
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.025 293.2
C (mp-66) <1 1 1> <0 1 0> 0.033 354.3
GaAs (mp-2534) <1 1 0> <1 0 0> 0.033 185.5
CaCO3 (mp-3953) <0 0 1> <0 1 0> 0.033 354.3
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.034 196.9
C (mp-48) <0 0 1> <0 1 0> 0.039 196.9
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.046 293.2
CdWO4 (mp-19387) <1 1 1> <1 0 0> 0.048 309.2
LiF (mp-1138) <1 1 0> <0 1 0> 0.049 118.1
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.050 185.5
Ge (mp-32) <1 0 0> <0 1 0> 0.056 196.9
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.057 309.2
NaCl (mp-22862) <1 0 0> <0 1 0> 0.058 196.9
NaCl (mp-22862) <1 1 0> <1 0 0> 0.060 185.5
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.065 221.9
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.066 185.5
GaTe (mp-542812) <1 0 0> <0 0 1> 0.066 221.9
DyScO3 (mp-31120) <1 0 1> <1 1 0> 0.067 219.9
SiC (mp-8062) <1 1 0> <1 0 0> 0.068 247.3
Ge (mp-32) <1 1 0> <1 0 0> 0.072 185.5
KCl (mp-23193) <1 1 0> <1 0 1> 0.075 289.2
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.088 185.5
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.091 289.2
Cu (mp-30) <1 0 0> <1 0 0> 0.093 309.2
CdS (mp-672) <1 0 1> <0 0 1> 0.098 295.9
LiF (mp-1138) <1 0 0> <0 1 0> 0.099 196.9
SiO2 (mp-6930) <0 0 1> <0 1 0> 0.104 354.3
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.110 61.8
InP (mp-20351) <1 0 0> <0 1 0> 0.111 315.0
CdS (mp-672) <1 1 0> <0 0 1> 0.119 147.9
TbScO3 (mp-31119) <1 0 1> <1 1 0> 0.120 219.9
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.122 96.4
SiC (mp-11714) <1 0 1> <0 1 0> 0.125 196.9
Mg (mp-153) <1 0 1> <1 0 0> 0.129 185.5
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.129 221.9
MgO (mp-1265) <1 1 1> <0 1 1> 0.130 251.4
ZnO (mp-2133) <1 0 0> <1 1 0> 0.135 293.2
Fe3O4 (mp-19306) <1 1 1> <0 1 1> 0.136 251.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.137 247.3
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.139 221.9
CdWO4 (mp-19387) <1 0 0> <0 1 1> 0.140 251.4
Te2W (mp-22693) <0 0 1> <1 1 0> 0.142 219.9
TeO2 (mp-2125) <1 0 1> <0 1 0> 0.149 78.7
WSe2 (mp-1821) <0 0 1> <0 1 1> 0.155 251.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 31 17 0 0 0
31 83 24 0 0 0
17 24 66 0 0 0
0 0 0 14 0 0
0 0 0 0 3 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
17.1 -5.7 -2.4 0 0 0
-5.7 15.4 -4.1 0 0 0
-2.4 -4.1 17.1 0 0 0
0 0 0 71.3 0 0
0 0 0 0 322.7 0
0 0 0 0 0 39
Shear Modulus GV
18 GPa
Bulk Modulus KV
40 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
39 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
40 GPa
Elastic Anisotropy
4.52
Poisson's Ratio
0.34

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
7.61 -0.00 0.00
-0.00 5.54 0.00
0.00 0.00 10.24
Dielectric Tensor εij (total)
46.08 -0.00 0.00
-0.00 11.37 0.00
0.00 0.00 12.86
Polycrystalline dielectric constant εpoly
(electronic contribution)
7.80
Polycrystalline dielectric constant εpoly
(total)
23.44
Refractive Index n
2.79
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsCrI2 (mp-675843) 0.6540 0.826 3
SrAgO2 (mp-997100) 0.7483 0.011 3
BaNiO2 (mp-18943) 0.4286 0.117 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Pd S
Final Energy/Atom
-5.0630 eV
Corrected Energy
-43.1579 eV
-43.1579 eV = -40.5041 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 202009
  • 63588
Submitted by
User remarks:
  • Barium palladium sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)