Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.160 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.482 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 159.8 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 300.8 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 225.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 266.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 225.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 266.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 226.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 266.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 225.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 150.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 213.1 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 225.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 266.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 266.4 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 225.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 266.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 213.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 91.9 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 150.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 213.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 213.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 225.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 -1> | 225.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 53.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 91.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 213.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 319.6 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 213.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 266.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 225.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 225.6 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 75.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 266.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 266.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 159.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 301.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 150.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 91.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 183.7 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 275.6 |
Al (mp-134) | <1 0 0> | <1 1 -1> | 213.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 225.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 266.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 266.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 275.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 266.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 92.3 |
CdTe (mp-406) | <1 0 0> | <1 1 -1> | 213.0 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 275.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Eu2Ru2O7 (mp-637431) | 0.5060 | 0.000 | 3 |
Y2Cr2O7 (mvc-14044) | 0.4456 | 0.031 | 3 |
Y2Co2O7 (mvc-14045) | 0.4764 | 0.080 | 3 |
Nd2Mo2O7 (mp-690122) | 0.4807 | 0.025 | 3 |
Eu2Mn2O7 (mp-769834) | 0.5015 | 0.000 | 3 |
La2Nb2N2O5 (mp-775911) | 0.4908 | 0.071 | 4 |
Mn2Hg2SF6 (mp-600275) | 0.5110 | 0.465 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.5112 | 0.000 | 4 |
Mn2Hg2SF6 (mp-556900) | 0.5116 | 0.465 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.5172 | 0.000 | 4 |
NaYb3Ti2(SbO7)2 (mp-695026) | 0.2107 | 0.074 | 5 |
GdTiCdSbO7 (mp-39684) | 0.3164 | 0.000 | 5 |
NaGd3Ti2(SbO7)2 (mp-40451) | 0.1289 | 0.000 | 5 |
NaNd3Ti2(SbO7)2 (mp-40484) | 0.2655 | 0.000 | 5 |
NaSm3Ti2(SbO7)2 (mp-40685) | 0.1794 | 0.004 | 5 |
NaYbTiNbO6F (mp-684861) | 0.2839 | 0.065 | 6 |
NaYTiNbO6F (mp-42599) | 0.3137 | 0.053 | 6 |
NaPrTiNbO6F (mp-42897) | 0.3212 | 0.035 | 6 |
NaCeTiNbO6F (mp-43055) | 0.3076 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.3221 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Dy_3 Ti_pv Sb O |
Final Energy/Atom-7.6427 eV |
Corrected Energy-355.9408 eV
-355.9408 eV = -336.2766 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)