Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.142 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToS(OF)2 + AsCl2F3 + AsF5 + SF6 |
Band Gap3.997 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 269.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 250.2 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 269.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 112.2 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 245.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 269.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.6 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 170.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 269.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 154.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.6 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 179.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 224.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 224.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 231.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 -1> | 245.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 166.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 154.4 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 154.4 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 170.5 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 227.3 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 -1> | 269.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 166.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 308.8 |
SiC (mp-7631) | <1 0 1> | <1 1 1> | 189.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 231.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 269.2 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 166.8 |
Mg (mp-153) | <1 0 1> | <1 1 -1> | 245.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 154.4 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 -1> | 269.2 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 -1> | 269.2 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 250.2 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 269.2 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 -1> | 269.2 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 224.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 112.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 250.2 |
Au (mp-81) | <1 0 0> | <0 1 1> | 227.3 |
Au (mp-81) | <1 1 0> | <1 0 0> | 224.5 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 166.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 250.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 231.6 |
C (mp-48) | <1 0 0> | <1 0 -1> | 269.2 |
C (mp-48) | <1 1 1> | <0 0 1> | 308.8 |
WSe2 (mp-1821) | <0 0 1> | <1 0 -1> | 269.2 |
WSe2 (mp-1821) | <1 0 0> | <1 1 -1> | 245.0 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 308.8 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 250.2 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 139.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al(HO)3 (mp-554883) | 0.6701 | 0.030 | 3 |
Al(HO)3 (mp-626502) | 0.6323 | 0.025 | 3 |
Al(HO)3 (mp-626431) | 0.6710 | 0.030 | 3 |
Al(HO)3 (mp-626074) | 0.6760 | 0.038 | 3 |
Al(HO)3 (mp-626103) | 0.6714 | 0.031 | 3 |
As2Cl3OF5 (mp-557417) | 0.5322 | 0.000 | 4 |
AsSOF9 (mp-556515) | 0.5640 | 0.044 | 4 |
SnP2Cl8O3 (mp-560891) | 0.5803 | 0.000 | 4 |
SbAsAuF9 (mp-758923) | 0.4915 | 0.013 | 4 |
AsCSF11 (mp-561235) | 0.6032 | 0.092 | 4 |
AsPCl3OF5 (mp-557360) | 0.5976 | 0.062 | 5 |
SnH16C4(Br3N)2 (mp-570137) | 0.5925 | 0.056 | 5 |
AsSXe2(OF3)3 (mp-560077) | 0.5503 | 0.041 | 5 |
FeH12C2N2F5 (mp-565741) | 0.6071 | 0.139 | 5 |
SnH16C4(NCl3)2 (mp-570712) | 0.5903 | 0.059 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.6639 | 0.118 | 6 |
SbH3CSCl6O (mp-561214) | 0.7374 | 0.120 | 6 |
AgBTe4C2(O3F10)2 (mp-557494) | 0.7381 | 0.161 | 6 |
AgBTe4C(OF4)5 (mp-559834) | 0.6802 | 0.085 | 6 |
AsC4S2Cl2O2F13 (mp-560424) | 0.7217 | 0.226 | 6 |
SbTe7SXeCl(OF4)9 (mp-581488) | 0.6501 | 0.043 | 7 |
SbTe7SXeCl(OF4)9 (mp-560359) | 0.7345 | 0.043 | 7 |
SbTe6H12C4N(OF5)6 (mp-709549) | 0.7283 | 0.281 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: As S Cl O F |
Final Energy/Atom-4.2254 eV |
Corrected Energy-224.8201 eV
Uncorrected energy = -202.8201 eV
Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV
Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV
Composition-based energy adjustment (-0.462 eV/atom x 32.0 atoms) = -14.7840 eV
Composition-based energy adjustment (-0.614 eV/atom x 4.0 atoms) = -2.4560 eV
Corrected energy = -224.8201 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)