material

CaCN2

ID:

mp-4124

DOI:

10.17188/1207876


Tags: Calcium dinitridocarbonate Calcium cyanamide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.086 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.635 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 418451 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-7631) <0 0 1> <0 0 1> 0.000 107.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.001 107.9
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.001 227.9
CdTe (mp-406) <1 1 1> <0 0 1> 0.001 227.9
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.002 227.9
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.003 107.9
Si (mp-149) <1 1 1> <0 0 1> 0.003 155.9
InSb (mp-20012) <1 1 1> <0 0 1> 0.004 227.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.004 155.9
GaN (mp-804) <0 0 1> <0 0 1> 0.005 36.0
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.005 227.9
BN (mp-984) <1 1 1> <0 0 1> 0.008 203.9
GaAs (mp-2534) <1 1 1> <0 0 1> 0.009 227.9
Ni (mp-23) <1 1 0> <1 0 1> 0.009 226.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.010 83.9
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.011 48.0
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.014 119.9
AlN (mp-661) <1 1 0> <0 0 1> 0.015 299.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.017 191.9
CsI (mp-614603) <1 1 1> <0 0 1> 0.024 107.9
KCl (mp-23193) <1 0 0> <1 1 0> 0.025 287.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.026 143.9
Al (mp-134) <1 1 1> <0 0 1> 0.029 83.9
Ge (mp-32) <1 1 1> <0 0 1> 0.029 227.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.032 155.9
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.034 191.9
GaP (mp-2490) <1 1 1> <0 0 1> 0.034 155.9
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.038 276.8
MoS2 (mp-1434) <1 0 1> <0 0 1> 0.041 275.8
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.061 155.9
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.061 215.9
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.062 275.8
ZrO2 (mp-2858) <1 1 -1> <1 0 1> 0.065 226.5
GaAs (mp-2534) <1 1 0> <0 0 1> 0.067 323.8
NaCl (mp-22862) <1 1 1> <0 0 1> 0.069 227.9
Ni (mp-23) <1 1 1> <0 0 1> 0.075 83.9
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.077 179.9
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.078 131.9
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.081 287.8
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.084 299.8
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.084 221.4
TePb (mp-19717) <1 1 1> <0 0 1> 0.086 227.9
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.086 251.8
Cu (mp-30) <1 1 1> <0 0 1> 0.089 155.9
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.092 191.9
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.103 359.8
Ge (mp-32) <1 1 0> <0 0 1> 0.104 323.8
GdScO3 (mp-5690) <1 1 1> <1 1 0> 0.107 287.6
C (mp-48) <1 0 0> <0 0 1> 0.107 227.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.111 251.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
98 34 51 -5 0 0
34 98 51 5 0 0
51 51 199 0 0 0
-5 5 0 10 0 0
0 0 0 0 10 -5
0 0 0 0 -5 32
Compliance Tensor Sij (10-12Pa-1)
13.2 -3.7 -2.4 8.4 0 0
-3.7 13.2 -2.4 -8.4 0 0
-2.4 -2.4 6.3 0 0 0
8.4 -8.4 0 104.4 0 0
0 0 0 0 104.4 16.9
0 0 0 0 16.9 33.8
Shear Modulus GV
28 GPa
Bulk Modulus KV
74 GPa
Shear Modulus GR
17 GPa
Bulk Modulus KR
64 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
69 GPa
Elastic Anisotropy
3.45
Poisson's Ratio
0.35

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.71 -0.00 -0.00
-0.00 2.71 -0.00
-0.00 -0.00 4.62
Dielectric Tensor εij (total)
6.88 -0.00 -0.00
-0.00 6.88 -0.00
-0.00 -0.00 11.39
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.35
Polycrystalline dielectric constant εpoly
(total)
8.38
Refractive Index n
1.83
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MnCN2 (mp-12335) 0.1618 0.064 3
CdCN2 (mp-10969) 0.0350 0.000 3
MgCN2 (mp-9166) 0.1789 0.000 3
NaHF2 (mp-27837) 0.0442 0.000 3
SrCN2 (mp-12317) 0.1386 0.000 3
NaCNO (mp-546500) 0.2037 0.000 4
NaAg(CN)2 (mp-568422) 0.4885 0.217 4
NaCSN (mp-6633) 0.6647 0.000 4
KAg(CN)2 (mp-582994) 0.5930 0.191 4
KAu(CN)2 (mp-672348) 0.5735 0.117 4
NaN3 (mp-22003) 0.2678 0.000 2
NaN3 (mp-570538) 0.3603 0.000 2
NaN3 (mp-1066400) 0.1334 0.002 2
NaN3 (mp-1064952) 0.3452 0.002 2
LiN3 (mp-2659) 0.3431 0.000 2
Sr2LiCBr3N2 (mp-569782) 0.6827 0.000 5
LiEu2CBr3N2 (mp-568863) 0.6884 0.000 5
K2NaAg3(CN)6 (mp-6855) 0.6728 0.207 5
AgSbH2C2(NF3)2 (mp-690698) 0.7426 0.160 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv C N
Final Energy/Atom
-7.8683 eV
Corrected Energy
-32.1953 eV
Uncorrected energy = -31.4733 eV Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV Corrected energy = -32.1953 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 25763
  • 26677
  • 418451
  • 28319
  • 31100
Submitted by
User remarks:
  • Calcium cyanamide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)