material

Rb2CO3

ID:

mp-4138

DOI:

10.17188/1207884


Tags: Rubidium carbonate Dirubidium carbonate - gamma

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.085 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.287 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 14155 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.005 207.2
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.006 182.0
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.006 182.0
SiC (mp-11714) <1 0 0> <1 0 -1> 0.007 94.0
PbS (mp-21276) <1 1 0> <0 0 1> 0.007 304.4
YAlO3 (mp-3792) <1 1 1> <1 0 -1> 0.010 188.0
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.011 60.9
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.012 304.4
YVO4 (mp-19133) <0 0 1> <1 0 1> 0.015 103.6
LiF (mp-1138) <1 0 0> <0 1 0> 0.017 318.5
ZnO (mp-2133) <0 0 1> <0 1 0> 0.018 273.0
Ni (mp-23) <1 0 0> <1 0 1> 0.019 207.2
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.019 270.8
LiGaO2 (mp-5854) <0 0 1> <1 0 -1> 0.019 281.9
Cu (mp-30) <1 0 0> <1 0 1> 0.020 103.6
Fe2O3 (mp-24972) <1 0 0> <1 0 -1> 0.020 281.9
CdWO4 (mp-19387) <0 1 1> <1 0 -1> 0.021 281.9
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.024 182.7
C (mp-66) <1 1 0> <0 0 1> 0.025 182.7
InP (mp-20351) <1 1 0> <0 0 1> 0.026 304.4
ZnO (mp-2133) <1 1 1> <0 1 0> 0.029 318.5
AlN (mp-661) <0 0 1> <0 1 0> 0.029 227.5
TeO2 (mp-2125) <0 0 1> <1 1 1> 0.033 226.3
BN (mp-984) <1 0 0> <1 0 0> 0.034 78.0
Te2Mo (mp-602) <0 0 1> <0 1 0> 0.035 273.0
AlN (mp-661) <1 1 0> <1 1 0> 0.035 270.8
AlN (mp-661) <1 1 1> <0 1 0> 0.036 227.5
KCl (mp-23193) <1 0 0> <1 0 1> 0.036 207.2
Cu (mp-30) <1 1 0> <0 0 1> 0.038 182.7
ZnO (mp-2133) <1 1 0> <0 1 1> 0.041 152.0
C (mp-48) <1 0 1> <0 1 0> 0.041 182.0
Cu (mp-30) <1 1 1> <0 0 1> 0.042 182.7
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.046 233.9
AlN (mp-661) <1 0 1> <0 1 1> 0.046 304.1
AlN (mp-661) <1 0 0> <1 0 -1> 0.047 94.0
BN (mp-984) <0 0 1> <1 1 0> 0.049 180.5
CaF2 (mp-2741) <1 1 0> <0 1 1> 0.052 304.1
Au (mp-81) <1 1 1> <0 0 1> 0.052 60.9
ZnO (mp-2133) <1 0 1> <0 1 0> 0.054 136.5
GaSe (mp-1943) <1 0 1> <0 1 0> 0.054 136.5
MgO (mp-1265) <1 0 0> <0 0 1> 0.055 182.7
LaF3 (mp-905) <1 0 1> <1 0 -1> 0.056 281.9
MoSe2 (mp-1634) <1 0 1> <0 1 0> 0.059 318.5
GaP (mp-2490) <1 1 0> <0 1 1> 0.060 304.1
CdS (mp-672) <1 0 0> <0 1 1> 0.067 228.0
LiF (mp-1138) <1 1 1> <1 0 0> 0.068 233.9
C (mp-66) <1 0 0> <0 0 1> 0.069 304.4
NdGaO3 (mp-3196) <1 0 0> <0 1 1> 0.071 304.1
SiC (mp-11714) <1 1 0> <0 1 0> 0.073 318.5
BN (mp-984) <1 0 1> <1 1 0> 0.074 180.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
26 20 18 0 5 0
20 46 20 0 3 0
18 20 59 0 7 0
0 0 0 17 0 3
5 3 7 0 7 0
0 0 0 3 0 7
Compliance Tensor Sij (10-12Pa-1)
68 -24.2 -9.4 0 -26.6 0
-24.2 34.3 -5.1 0 7.6 0
-9.4 -5.1 23.9 0 -17.7 0
0 0 0 61.1 0 -24.3
-26.6 7.6 -17.7 0 186.7 0
0 0 0 -24.3 0 155.7
Shear Modulus GV
11 GPa
Bulk Modulus KV
27 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
20 GPa
Shear Modulus GVRH
10 GPa
Bulk Modulus KVRH
24 GPa
Elastic Anisotropy
2.20
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na2CO3 (mp-3070) 0.4872 0.006 3
BaCO3 (mp-675324) 0.4594 0.076 3
K2CO3 (mp-554072) 0.4491 0.002 3
Rb2CO3 (mp-555692) 0.5067 0.002 3
K2CO3 (mp-3963) 0.2247 0.000 3
NaMnBO3 (mp-776039) 0.5744 0.018 4
BaNaBO3 (mp-6660) 0.5975 0.000 4
Eu3BWO9 (mp-566088) 0.5898 0.000 4
NaSrBO3 (mp-556695) 0.6060 0.000 4
BaCa(CO3)2 (mp-644852) 0.4809 0.014 4
NaSbCO2F3 (mp-554239) 0.5848 0.031 5
Na3MoH6(CO2)6 (mp-579529) 0.6440 0.105 5
NaSbCO2F3 (mp-554716) 0.5722 0.031 5
CdH24C4(BrN2)6 (mp-707501) 0.6557 0.002 5
NaCdH3(CO2)3 (mp-557366) 0.4733 0.107 5
FeH16C4S4(N4Cl)2 (mp-723036) 0.6260 0.101 6
CdH16C4S4(N4Cl)2 (mp-699261) 0.6955 0.033 6
CdH4CN2Cl2O (mp-697033) 0.6147 0.001 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv C O
Final Energy/Atom
-6.0802 eV
Corrected Energy
-154.1690 eV
Uncorrected energy = -145.9250 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Corrected energy = -154.1690 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 14155
  • 414123
Submitted by
User remarks:
  • Rubidium carbonate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)