material

Li2ZrO3

ID:

mp-4156

DOI:

10.17188/1207897


Tags: Dilithium zirconate Dilithium zirconium trioxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.048 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.03 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.841 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/c [15]
Hall
-C 2yc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 94893 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <1 0 0> <0 1 0> 220.6
LaAlO3 (mp-2920) <1 1 1> <1 0 1> 248.4
AlN (mp-661) <0 0 1> <0 1 0> 110.3
AlN (mp-661) <1 0 1> <0 1 0> 137.9
CeO2 (mp-20194) <1 1 1> <0 1 0> 303.4
GaAs (mp-2534) <1 0 0> <1 0 1> 165.6
BaF2 (mp-1029) <1 0 0> <1 0 -1> 167.1
BaF2 (mp-1029) <1 1 0> <1 1 1> 174.5
BaF2 (mp-1029) <1 1 1> <1 0 -1> 278.6
GaN (mp-804) <1 1 1> <0 1 0> 220.6
SiO2 (mp-6930) <1 0 1> <0 0 1> 349.0
SiO2 (mp-6930) <1 1 0> <0 1 1> 284.9
KCl (mp-23193) <1 0 0> <1 0 1> 82.8
DyScO3 (mp-31120) <0 0 1> <0 1 0> 220.6
DyScO3 (mp-31120) <1 1 0> <0 1 0> 330.9
InAs (mp-20305) <1 0 0> <0 1 0> 110.3
ZnSe (mp-1190) <1 0 0> <1 0 1> 165.6
KTaO3 (mp-3614) <1 1 0> <0 1 1> 284.9
LiF (mp-1138) <1 1 0> <0 1 0> 248.2
LiF (mp-1138) <1 1 1> <0 1 0> 358.5
TePb (mp-19717) <1 1 1> <0 0 1> 149.6
Ag (mp-124) <1 0 0> <0 0 1> 349.0
Ag (mp-124) <1 1 0> <0 1 0> 220.6
Ag (mp-124) <1 1 1> <0 1 0> 330.9
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 137.9
GaSe (mp-1943) <0 0 1> <0 1 0> 248.2
BN (mp-984) <1 0 0> <0 1 0> 193.0
BN (mp-984) <1 1 1> <0 1 1> 284.9
LiNbO3 (mp-3731) <1 1 0> <1 0 1> 248.4
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 165.5
Al (mp-134) <1 0 0> <1 0 1> 82.8
Al (mp-134) <1 1 0> <0 1 1> 284.9
Al (mp-134) <1 1 1> <0 1 0> 358.5
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 199.4
LiGaO2 (mp-5854) <0 1 0> <0 1 1> 227.9
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 249.3
LiGaO2 (mp-5854) <1 0 1> <0 1 0> 220.6
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 49.9
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 149.6
LaAlO3 (mp-2920) <1 1 0> <1 0 1> 248.4
AlN (mp-661) <1 0 0> <0 1 0> 110.3
AlN (mp-661) <1 1 0> <0 0 1> 249.3
AlN (mp-661) <1 1 1> <0 0 1> 349.0
CeO2 (mp-20194) <1 0 0> <0 0 1> 149.6
CeO2 (mp-20194) <1 1 0> <0 0 1> 249.3
GaN (mp-804) <0 0 1> <0 0 1> 249.3
GaN (mp-804) <1 0 0> <1 1 -1> 248.7
GaN (mp-804) <1 0 1> <0 1 0> 220.6
GaN (mp-804) <1 1 0> <0 0 1> 199.4
SiO2 (mp-6930) <0 0 1> <0 1 0> 358.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
289 83 48 0 -16 0
83 240 57 0 6 0
48 57 135 0 -42 0
0 0 0 59 0 19
-16 6 -42 0 55 0
0 0 0 19 0 60
Compliance Tensor Sij (10-12Pa-1)
4 -1.2 -0.6 0 0.8 0
-1.2 5.3 -2.8 0 -3.1 0
-0.6 -2.8 11.6 0 9 0
0 0 0 18.9 0 -6.1
0.8 -3.1 9 0 25.7 0
0 0 0 -6.1 0 18.7
Shear Modulus GV
66 GPa
Bulk Modulus KV
115 GPa
Shear Modulus GR
51 GPa
Bulk Modulus KR
86 GPa
Shear Modulus GVRH
59 GPa
Bulk Modulus KVRH
101 GPa
Elastic Anisotropy
1.81
Poisson's Ratio
0.26

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.58 -0.00 0.10
-0.00 4.24 0.00
0.10 0.00 3.88
Dielectric Tensor εij (total)
39.70 -0.00 18.04
-0.00 23.48 -0.00
18.04 -0.00 51.09
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.23
Polycrystalline dielectric constant εpoly
(total)
38.09
Refractive Index n
2.06
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li5Ni7O12 (mp-771626) 0.1851 0.015 3
Li7Fe5O12 (mp-771617) 0.1669 0.016 3
Li2HfO3 (mp-755352) 0.1907 0.000 3
Li3SbS4 (mp-752426) 0.1662 0.062 3
Li2TiO3 (mp-760017) 0.1748 0.156 3
Li5Fe3(SnO5)2 (mp-769826) 0.1384 0.019 4
Li3Mn4CrO8 (mp-771116) 0.1757 0.039 4
Li11Nb4(Ni3O8)3 (mp-769524) 0.1595 0.062 4
Li3MnCr4O8 (mp-769831) 0.1772 0.101 4
Li3Mn4VO8 (mp-771401) 0.1738 0.082 4
Te2Au (mp-1662) 0.4404 0.018 2
NaTe3 (mp-28478) 0.3244 0.000 2
LiTe3 (mp-27466) 0.3290 0.009 2
Sb2Te3 (mp-1080789) 0.4913 0.129 2
Te2Au (mp-567525) 0.4492 0.018 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.4989 0.139 5
Hg (mp-982872) 0.7121 0.020 1
Sb (mp-632286) 0.5843 0.059 1
Bi (mp-567379) 0.7383 0.059 1
Te (mp-570459) 0.5893 0.044 1
Te (mp-105) 0.6122 0.047 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Crystalline powders of Li2ZrO3 were prepared by gelling ZrCl4 and CH3COOLi with NH4OH at 50 C, at different pH values (5, 7 and 8) and for different times (3, 12 and 24 h), then drying and calcining. [...]
A new approach has been developed to produce high purity, fine grained lithium orthosilicate (Li4SiO4) and lithium metazirconate (Li2ZrO3). This technique is based on an organometallic process 1n whic [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Li2ZrO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Zr_sv O
Final Energy/Atom
-7.2316 eV
Corrected Energy
-90.9013 eV
Uncorrected energy = -86.7793 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -90.9013 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 291154
  • 94897
  • 191166
  • 94895
  • 94896
  • 94894
  • 94893
Submitted by
User remarks:
  • Dilithium zirconium trioxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)