Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.307 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSi2N2O + NdAlO3 + Al2O3 + Nd2SiO5 |
Band Gap3.379 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 280.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 291.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 97.3 |
GaAs (mp-2534) | <1 1 0> | <1 -1 0> | 137.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 291.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 -1 0> | 137.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 168.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 168.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 97.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 0> | 137.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 224.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 168.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 280.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 224.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 159.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 194.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 97.3 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 0> | 137.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 291.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 318.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 291.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 238.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 318.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 318.4 |
BN (mp-984) | <1 0 0> | <1 1 1> | 97.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 241.1 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 238.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 168.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 238.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 168.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 224.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 168.0 |
Al (mp-134) | <1 0 0> | <1 1 1> | 97.3 |
Al (mp-134) | <1 1 0> | <1 -1 0> | 137.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 224.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 318.4 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 97.2 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 291.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 168.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 224.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 291.5 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 291.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 318.4 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 224.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 318.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 224.0 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 160.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 -1 0> | 137.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9V14O35 (mp-850769) | 0.7060 | 0.049 | 3 |
Na9V14O35 (mp-578824) | 0.6611 | 0.000 | 3 |
AgAsO3 (mp-558950) | 0.7225 | 0.026 | 3 |
CaSnS3 (mp-866629) | 0.7091 | 0.184 | 3 |
K4Zn(WO4)3 (mp-622489) | 0.6540 | 0.020 | 4 |
LiMn2(PO4)2 (mp-778730) | 0.6409 | 0.027 | 4 |
K4Mn(MoO4)3 (mp-566918) | 0.6462 | 0.116 | 4 |
SrNi2(PO4)2 (mp-19647) | 0.6471 | 0.030 | 4 |
Ca3Mg3(PO4)4 (mp-646967) | 0.5661 | 0.017 | 4 |
Na3Ca2Fe5(SiO3)10 (mp-735984) | 0.7444 | 0.146 | 5 |
Li7MnP4O14F (mp-762708) | 0.7247 | 0.151 | 5 |
Li7FeP4O14F (mp-762690) | 0.7317 | 0.126 | 5 |
Na2SnGe2(HO4)2 (mp-757981) | 0.7114 | 0.000 | 5 |
Ca10TaTi8Al(SiO5)10 (mp-696633) | 0.6327 | 0.292 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.7359 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Al Si N O |
Final Energy/Atom-7.9141 eV |
Corrected Energy-381.2228 eV
Uncorrected energy = -364.0478 eV
Composition-based energy adjustment (-0.687 eV/atom x 25.0 atoms) = -17.1750 eV
Corrected energy = -381.2228 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)