material

V(CrC)2

ID:

mp-4253

DOI:

10.17188/1208005


Tags: Chromium vanadium carbide (2/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.180 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.083 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cr7C3 + Cr3C2 + V6C5
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <0 1 0> 0.005 161.7
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.008 222.3
MgO (mp-1265) <1 0 0> <0 1 0> 0.017 181.9
WS2 (mp-224) <1 0 0> <1 1 0> 0.023 136.5
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.026 80.8
LiF (mp-1138) <1 1 0> <0 1 0> 0.027 141.5
MgAl2O4 (mp-3536) <1 1 0> <0 1 0> 0.029 282.9
Al (mp-134) <1 1 1> <0 1 1> 0.032 198.2
MgAl2O4 (mp-3536) <1 1 1> <0 1 1> 0.032 231.2
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.041 280.9
TiO2 (mp-390) <1 0 0> <0 1 0> 0.051 222.3
Ni (mp-23) <1 1 0> <0 1 0> 0.052 121.3
KTaO3 (mp-3614) <1 1 1> <0 1 1> 0.055 198.2
ZnO (mp-2133) <0 0 1> <0 1 1> 0.068 66.1
Al (mp-134) <1 0 0> <0 1 0> 0.083 80.8
Bi2Te3 (mp-34202) <0 0 1> <0 1 0> 0.084 222.3
AlN (mp-661) <1 0 1> <0 1 0> 0.087 161.7
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.090 80.8
AlN (mp-661) <1 1 1> <0 0 1> 0.094 313.5
CdS (mp-672) <1 0 0> <0 1 0> 0.103 202.1
Te2Mo (mp-602) <1 1 0> <1 0 1> 0.110 280.9
ZnO (mp-2133) <1 1 1> <0 0 1> 0.111 156.8
ZnSe (mp-1190) <1 1 0> <0 1 0> 0.125 323.3
BN (mp-984) <1 0 0> <1 0 1> 0.128 210.7
SiC (mp-11714) <1 1 0> <1 1 1> 0.134 219.2
C (mp-66) <1 0 0> <0 1 0> 0.137 101.0
ZnO (mp-2133) <1 0 0> <0 1 0> 0.138 121.3
CdWO4 (mp-19387) <0 1 0> <0 1 1> 0.139 132.1
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.140 262.7
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.154 303.1
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.154 130.4
SiC (mp-7631) <1 0 0> <1 0 1> 0.154 140.5
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.160 287.4
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.161 195.6
Mg (mp-153) <0 0 1> <0 1 1> 0.162 231.2
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.173 182.9
Cu (mp-30) <1 1 1> <0 1 0> 0.178 202.1
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.183 156.8
GaAs (mp-2534) <1 1 0> <0 1 0> 0.187 323.3
KCl (mp-23193) <1 0 0> <0 1 1> 0.190 165.2
TeO2 (mp-2125) <1 0 0> <0 0 1> 0.194 209.0
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.195 202.1
ZnO (mp-2133) <1 1 0> <0 0 1> 0.198 209.0
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.212 156.8
NdGaO3 (mp-3196) <1 0 1> <0 1 0> 0.219 161.7
NdGaO3 (mp-3196) <1 0 0> <0 1 1> 0.226 132.1
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.231 303.1
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.235 261.3
TePb (mp-19717) <1 1 0> <0 0 1> 0.244 182.9
TiO2 (mp-390) <0 0 1> <0 1 1> 0.254 132.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
470 214 202 0 0 0
214 475 166 0 0 0
202 166 511 0 0 0
0 0 0 198 0 0
0 0 0 0 155 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
3 -1 -0.8 0 0 0
-1 2.7 -0.5 0 0 0
-0.8 -0.5 2.4 0 0 0
0 0 0 5.1 0 0
0 0 0 0 6.4 0
0 0 0 0 0 24.2
Shear Modulus GV
137 GPa
Bulk Modulus KV
291 GPa
Shear Modulus GR
101 GPa
Bulk Modulus KR
291 GPa
Shear Modulus GVRH
119 GPa
Bulk Modulus KVRH
291 GPa
Elastic Anisotropy
1.82
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiFeF3 (mp-777362) 0.2200 0.088 3
PrLuSe3 (mp-13326) 0.3375 0.000 3
NdLuSe3 (mp-13327) 0.3128 0.000 3
NdLuS3 (mp-1080801) 0.3304 0.000 3
CeLuS3 (mp-1092225) 0.3071 0.011 3
Ca2SbMoO6 (mvc-4146) 0.6288 0.016 4
PrMg(AgO3)2 (mvc-9234) 0.5829 0.106 4
CaPr(AgO3)2 (mvc-9268) 0.5765 0.088 4
HoMgMn2O6 (mvc-10195) 0.6245 0.089 4
CaPr(SnO3)2 (mvc-9344) 0.6065 0.132 4
As3Rh (mp-8182) 0.6185 0.000 2
Al2O3 (mp-642363) 0.3583 0.280 2
Cr3C2 (mp-570112) 0.1614 0.030 2
Ga2O3 (mp-13134) 0.2341 0.284 2
Fe2O3 (mp-1078361) 0.1843 0.704 2
LiLaNdSbO6 (mp-776091) 0.7250 0.006 5
CaLaFeBiO6 (mvc-8967) 0.6835 0.057 5
CaLaFeAgO6 (mvc-8977) 0.7230 0.054 5
LaMgFeSnO6 (mvc-9082) 0.7261 0.290 5
CaLaCrBiO6 (mvc-9978) 0.7213 0.198 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Cr_pv C
Final Energy/Atom
-9.5486 eV
Corrected Energy
-95.4859 eV
-95.4859 eV = -95.4859 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 20297
  • 43191
Submitted by
User remarks:
  • Chromium vanadium carbide (2/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)