Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.284 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.250 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 1> | 161.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 135.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 101.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 161.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 147.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 202.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 115.6 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 210.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 86.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 144.4 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 221.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 346.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 144.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 225.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 161.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 161.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 147.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 221.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 144.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 28.9 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 241.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 28.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 144.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 317.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 202.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 260.0 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 202.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 317.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 210.5 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 221.1 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 202.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 241.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 225.6 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 241.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 260.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.6 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 147.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 317.8 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 221.1 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 294.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 147.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 288.9 |
Te2W (mp-22693) | <1 1 0> | <0 1 1> | 221.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 288.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 101.2 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 202.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 317.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 86.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.03 | 0.00 | 0.00 |
0.00 | 3.44 | 0.00 |
0.00 | 0.00 | 3.62 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.79 | 0.00 | 0.00 |
0.00 | 8.60 | 0.00 |
0.00 | 0.00 | 13.61 |
Polycrystalline dielectric constant
εpoly∞
3.36
|
Polycrystalline dielectric constant
εpoly
10.00
|
Refractive Index n1.83 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2TeO6 (mp-8504) | 0.5157 | 0.000 | 3 |
Na2GeF6 (mp-17297) | 0.4900 | 0.000 | 3 |
CaTeO4 (mp-12221) | 0.2930 | 0.000 | 3 |
BaTeO4 (mp-754967) | 0.3310 | 0.000 | 3 |
Na2TiF6 (mp-556024) | 0.4852 | 0.000 | 3 |
InAg(WO4)2 (mp-614383) | 0.4213 | 0.018 | 4 |
Na2W(OF2)2 (mp-541649) | 0.4024 | 0.000 | 4 |
NaFe(WO4)2 (mp-25534) | 0.4750 | 0.003 | 4 |
NaIn(WO4)2 (mp-25649) | 0.4449 | 0.000 | 4 |
SrLiCoF6 (mp-567464) | 0.5001 | 0.017 | 4 |
BiO2 (mvc-4364) | 0.7119 | 0.186 | 2 |
SbO2 (mvc-2949) | 0.5701 | 0.272 | 2 |
BiO2 (mvc-5760) | 0.6520 | 0.079 | 2 |
BiO2 (mvc-9397) | 0.7144 | 0.175 | 2 |
TiO2 (mp-1439) | 0.7222 | 0.032 | 2 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Te O |
Final Energy/Atom-5.9201 eV |
Corrected Energy-153.3184 eV
-153.3184 eV = -142.0818 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)