Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.837 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSmSnAu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 78.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 58.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 144.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 164.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 250.4 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 196.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 180.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 313.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 98.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 187.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 58.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 287.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 78.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 255.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 287.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 262.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 373.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 255.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 253.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 287.9 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 287.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 250.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 205.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 325.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 253.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 328.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 164.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 58.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 58.9 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 262.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 216.9 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 262.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 255.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 98.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 187.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 98.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 137.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 255.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 98.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 98.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 255.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 329.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 289.1 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 250.4 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 262.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 176.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 216.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 314.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 78.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyCuPb (mp-22085) | 0.0724 | 0.000 | 3 |
GdSnAu (mp-20434) | 0.0430 | 0.015 | 3 |
YCuPb (mp-20865) | 0.0654 | 0.000 | 3 |
CaBiAu (mp-1018657) | 0.1018 | 0.048 | 3 |
TbCuPb (mp-20290) | 0.0760 | 0.000 | 3 |
LiSm(CuP)2 (mp-973019) | 0.7349 | 0.000 | 4 |
LiYb(CuP)2 (mp-1024988) | 0.7326 | 0.000 | 4 |
EuTl2 (mp-30630) | 0.3618 | 0.000 | 2 |
MgGa2 (mp-30651) | 0.3975 | 0.005 | 2 |
EuIn2 (mp-636316) | 0.3861 | 0.000 | 2 |
YbIn2 (mp-568058) | 0.3723 | 0.000 | 2 |
CaIn2 (mp-21068) | 0.3568 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Sn_d Au |
Final Energy/Atom-4.8375 eV |
Corrected Energy-29.0253 eV
-29.0253 eV = -29.0253 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)