Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.667 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 279.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 226.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 172.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 232.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 243.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 172.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 216.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 156.5 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 186.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 86.4 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 122.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 365.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 156.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 365.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 312.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 365.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 254.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 86.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 208.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 232.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 278.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 173.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 259.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 345.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 302.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 173.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 312.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 243.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 172.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 156.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 139.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 317.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 312.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 121.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 86.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 129.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 278.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 330.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 172.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 17.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 86.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 129.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 216.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 86.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 191.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 330.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
163 | 32 | 47 | -0 | 0 | 0 |
32 | 163 | 47 | 0 | 0 | 0 |
47 | 47 | 40 | 0 | 0 | 0 |
-0 | 0 | 0 | 30 | 0 | 0 |
0 | 0 | 0 | 0 | 30 | -0 |
0 | 0 | 0 | 0 | -0 | 26 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.7 | 2 | -13.7 | 0 | 0 | 0 |
2 | 9.7 | -13.7 | 0 | 0 | 0 |
-13.7 | -13.7 | 57 | 0 | 0 | 0 |
0 | 0 | 0 | 33.2 | 0 | 0 |
0 | 0 | 0 | 0 | 33.2 | 0 |
0 | 0 | 0 | 0 | 0 | 38.3 |
Shear Modulus GV33 GPa |
Bulk Modulus KV69 GPa |
Shear Modulus GR21 GPa |
Bulk Modulus KR39 GPa |
Shear Modulus GVRH27 GPa |
Bulk Modulus KVRH54 GPa |
Elastic Anisotropy3.75 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pb2ClOF (mp-23104) | 0.6770 | 0.000 | 4 |
K2LiInAs2 (mp-505431) | 0.6980 | 0.000 | 4 |
K2NaInP2 (mp-21511) | 0.7479 | 0.000 | 4 |
La3Cu4(P2O)2 (mp-6309) | 0.5192 | 0.000 | 4 |
K2LiAlP2 (mp-6450) | 0.7478 | 0.000 | 4 |
ThZn4 (mp-536) | 0.4172 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.4224 | 0.000 | 2 |
BaGa4 (mp-335) | 0.4143 | 0.000 | 2 |
EuGa4 (mp-21884) | 0.4259 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.3987 | 0.000 | 2 |
Eu(NiSb)2 (mp-570308) | 0.1145 | 0.000 | 3 |
Eu(FeSi)2 (mp-582357) | 0.1074 | 0.000 | 3 |
Sr(NiGe)2 (mp-3207) | 0.0906 | 0.000 | 3 |
La(CoGe)2 (mp-19939) | 0.0681 | 0.000 | 3 |
Nd(NiSb)2 (mp-568161) | 0.1306 | 0.052 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points104 |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv As Sr_sv |
Final Energy/Atom-5.1778 eV |
Corrected Energy-25.8891 eV
-25.8891 eV = -25.8891 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)