Final Magnetic Moment0.079 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.268 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3Se2 + Tl5Se3 + Ni3Se4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 75.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 74.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 75.6 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 75.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 222.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 302.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 196.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 196.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 209.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 136.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 272.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 209.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 45.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 166.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 318.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 148.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 196.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 242.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 242.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 196.8 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 209.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 222.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 209.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 222.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 218.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 227.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 60.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 287.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 209.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 136.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 272.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 136.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 227.1 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 148.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 302.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 136.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 257.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 209.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 272.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 272.6 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 296.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 302.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 257.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 333.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 261.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 314.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
71 | 26 | 31 | 0 | 0 | 0 |
26 | 71 | 31 | 0 | 0 | 0 |
31 | 31 | 44 | 0 | 0 | 0 |
0 | 0 | 0 | 11 | 0 | 0 |
0 | 0 | 0 | 0 | 11 | 0 |
0 | 0 | 0 | 0 | 0 | 19 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
20.5 | -1.8 | -13.3 | 0 | 0 | 0 |
-1.8 | 20.5 | -13.3 | 0 | 0 | 0 |
-13.3 | -13.3 | 41.3 | 0 | 0 | 0 |
0 | 0 | 0 | 91.5 | 0 | 0 |
0 | 0 | 0 | 0 | 91.5 | 0 |
0 | 0 | 0 | 0 | 0 | 53.3 |
Shear Modulus GV15 GPa |
Bulk Modulus KV41 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR39 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH40 GPa |
Elastic Anisotropy0.67 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K(CoSe)2 (mp-4668) | 0.0644 | 0.026 | 3 |
K(CoSe)2 (mp-1000625) | 0.0587 | 0.026 | 3 |
Ba(MnAs)2 (mp-15608) | 0.1437 | 0.000 | 3 |
Ba(MnP)2 (mp-19857) | 0.1538 | 0.003 | 3 |
K(NiSe)2 (mp-1070216) | 0.0824 | 0.051 | 3 |
KLiZnS2 (mp-774907) | 0.2064 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.6553 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.6648 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.3103 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.5129 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.4967 | 0.125 | 2 |
NbS2 (mp-1008860) | 0.7436 | 0.269 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Ni_pv Se |
Final Energy/Atom-4.4505 eV |
Corrected Energy-23.1967 eV
Uncorrected energy = -22.2527 eV
Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV
Corrected energy = -23.1967 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)