Final Magnetic Moment0.044 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.350 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.534 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 219.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 109.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 109.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 219.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 109.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 135.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 135.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 109.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 219.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 219.3 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 109.6 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 135.5 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 174.3 |
Au (mp-81) | <1 1 0> | <0 0 1> | 219.3 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 219.3 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 109.6 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 219.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2U2O7 (mp-675710) | 0.6148 | 0.005 | 3 |
Rb2U2O7 (mp-674373) | 0.5966 | 0.008 | 3 |
Rb8U9O31 (mp-683981) | 0.3558 | 0.010 | 3 |
K2U7O22 (mp-540610) | 0.5049 | 0.038 | 3 |
Rb4U5O17 (mp-558239) | 0.1727 | 0.004 | 3 |
Rb2U3(TeO7)2 (mp-542501) | 0.5546 | 0.000 | 4 |
KUNbO6 (mp-554887) | 0.6827 | 0.000 | 4 |
Cs2U3(TeO7)2 (mp-562366) | 0.5350 | 0.000 | 4 |
K4U5Te2O21 (mp-556212) | 0.7103 | 0.000 | 4 |
K2U3(TeO7)2 (mp-11887) | 0.5052 | 0.000 | 4 |
UO3 (mp-616580) | 0.6844 | 0.134 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv U O |
Final Energy/Atom-8.4355 eV |
Corrected Energy-924.0122 eV
Uncorrected energy = -877.2962 eV
Composition-based energy adjustment (-0.687 eV/atom x 68.0 atoms) = -46.7160 eV
Corrected energy = -924.0122 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)