Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.686 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.633 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPa3 [205] |
Hall-P 2ac 2ab 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 275.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 68.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 97.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 206.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 275.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 275.2 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 291.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 275.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 68.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 97.3 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 119.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 119.2 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 291.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 68.8 |
C (mp-66) | <1 1 0> | <1 1 0> | 291.9 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 275.2 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 97.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 291.9 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 194.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 1> | 238.4 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 291.9 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 291.9 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 291.9 |
Au (mp-81) | <1 0 0> | <1 0 0> | 68.8 |
Au (mp-81) | <1 1 1> | <1 1 1> | 119.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 68.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 97.3 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 275.2 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 275.2 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 291.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 291.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 206.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 137.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 194.6 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 68.8 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 97.3 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 291.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 97.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 119.2 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 68.8 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 97.3 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 275.2 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 194.6 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 275.2 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 206.4 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 275.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 68.8 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 275.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 275.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
36 | 24 | 24 | 0 | 0 | 0 |
24 | 36 | 24 | 0 | 0 | 0 |
24 | 24 | 36 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 13 | 0 |
0 | 0 | 0 | 0 | 0 | 13 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
60 | -23.9 | -23.9 | 0 | 0 | 0 |
-23.9 | 60 | -23.9 | 0 | 0 | 0 |
-23.9 | -23.9 | 60 | 0 | 0 | 0 |
0 | 0 | 0 | 76.8 | 0 | 0 |
0 | 0 | 0 | 0 | 76.8 | 0 |
0 | 0 | 0 | 0 | 0 | 76.8 |
Shear Modulus GV10 GPa |
Bulk Modulus KV28 GPa |
Shear Modulus GR9 GPa |
Bulk Modulus KR28 GPa |
Shear Modulus GVRH10 GPa |
Bulk Modulus KVRH28 GPa |
Elastic Anisotropy0.77 |
Poisson's Ratio0.35 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv N O |
Final Energy/Atom-6.4970 eV |
Corrected Energy-250.3793 eV
Uncorrected energy = -233.8913 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -250.3793 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)