material

CaAu2

ID:

mp-443

DOI:

10.17188/1208149


Tags: Calcium gold (1/2) Gold calcium (2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.710 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.37 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Imma [74]
Hall
-I 2b 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 55542 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <1 1 1> <1 0 0> 0.002 237.1
NdGaO3 (mp-3196) <0 1 0> <0 1 1> 0.003 256.7
GaP (mp-2490) <1 1 0> <0 1 1> 0.009 256.7
Ag (mp-124) <1 1 0> <0 1 0> 0.019 194.7
CaF2 (mp-2741) <1 1 0> <0 1 1> 0.022 256.7
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.023 234.2
TiO2 (mp-2657) <1 0 1> <0 1 1> 0.026 51.3
Ni (mp-23) <1 1 1> <1 1 0> 0.029 212.8
LaF3 (mp-905) <1 0 0> <0 0 1> 0.034 267.7
YAlO3 (mp-3792) <1 1 1> <0 1 0> 0.037 311.5
Cu (mp-30) <1 0 0> <0 0 1> 0.039 234.2
CdTe (mp-406) <1 1 0> <0 1 1> 0.044 308.0
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.051 200.8
ZnO (mp-2133) <0 0 1> <1 1 0> 0.051 141.8
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.052 141.8
SiO2 (mp-6930) <1 0 1> <0 1 0> 0.052 350.4
BN (mp-984) <1 0 0> <0 0 1> 0.055 234.2
Te2W (mp-22693) <0 1 1> <0 0 1> 0.056 234.2
InSb (mp-20012) <1 1 0> <0 1 1> 0.056 308.0
C (mp-48) <0 0 1> <0 0 1> 0.058 167.3
MoS2 (mp-1434) <1 1 1> <1 1 1> 0.059 235.3
Au (mp-81) <1 1 0> <0 1 0> 0.063 194.7
Mg (mp-153) <1 0 1> <0 0 1> 0.063 301.1
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.066 141.8
GdScO3 (mp-5690) <0 0 1> <0 1 1> 0.068 256.7
Mg (mp-153) <1 0 0> <1 1 0> 0.072 283.7
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.073 272.5
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.076 237.1
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.076 237.1
TePb (mp-19717) <1 1 0> <0 1 1> 0.077 308.0
MgF2 (mp-1249) <1 1 0> <0 1 0> 0.079 311.5
GaSe (mp-1943) <0 0 1> <1 0 0> 0.083 237.1
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.087 200.8
GaTe (mp-542812) <1 0 1> <0 1 0> 0.087 194.7
Si (mp-149) <1 1 0> <0 1 1> 0.091 256.7
GaTe (mp-542812) <1 0 0> <1 0 0> 0.093 177.8
CeO2 (mp-20194) <1 1 0> <0 1 1> 0.098 256.7
C (mp-48) <1 0 0> <0 0 1> 0.098 133.8
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.098 167.3
SiC (mp-7631) <0 0 1> <0 1 0> 0.103 116.8
SiC (mp-11714) <0 0 1> <0 1 0> 0.104 116.8
CdS (mp-672) <1 1 0> <0 0 1> 0.106 100.4
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.106 334.6
KP(HO2)2 (mp-23959) <0 1 0> <0 1 1> 0.108 154.0
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.118 66.9
AlN (mp-661) <1 0 0> <0 0 1> 0.128 301.1
NaCl (mp-22862) <1 0 0> <0 1 0> 0.131 194.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.131 100.4
C (mp-66) <1 1 0> <1 0 0> 0.135 177.8
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.135 194.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
78 37 37 0 0 0
37 109 98 0 0 0
37 98 108 0 0 0
0 0 0 14 0 0
0 0 0 0 16 0
0 0 0 0 0 14
Compliance Tensor Sij (10-12Pa-1)
15.5 -3.1 -2.5 0 0 0
-3.1 51.4 -45.6 0 0 0
-2.5 -45.6 51.5 0 0 0
0 0 0 72.3 0 0
0 0 0 0 62.2 0
0 0 0 0 0 72.1
Shear Modulus GV
17 GPa
Bulk Modulus KV
71 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
67 GPa
Elastic Anisotropy
2.46
Poisson's Ratio
0.40

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScNiSn (mp-5186) 0.4728 0.009 3
CaSnAu (mp-1071278) 0.5053 0.013 3
CeZnAu (mp-13549) 0.4740 0.000 3
ScGePt (mp-1095253) 0.3979 0.000 3
ErSnPd (mp-1095377) 0.5039 0.035 3
YbAg2 (mp-568559) 0.2947 0.000 2
CeAu2 (mp-1077442) 0.2023 0.000 2
LaAu2 (mp-1072087) 0.3078 0.000 2
NdAg2 (mp-1072737) 0.2889 0.000 2
PrAu2 (mp-30415) 0.2168 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Au
Final Energy/Atom
-3.5611 eV
Corrected Energy
-21.3666 eV
Uncorrected energy = -21.3666 eV Corrected energy = -21.3666 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 55542
  • 58402
Submitted by
User remarks:
  • Calcium gold (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)