material

CaSiPt

ID:

mp-4478

DOI:

10.17188/1208180


Tags: Calcium platinum silicide (1/1/1) Calcium platinum silicide - I

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.973 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P213 [198]
Hall
P 2ac 2ab 3
Point Group
23
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 63555 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 0 0> <1 0 0> 0.000 163.1
MgO (mp-1265) <1 1 0> <1 1 0> 0.000 230.6
SiC (mp-8062) <1 0 0> <1 0 0> 0.000 326.1
Al (mp-134) <1 0 0> <1 0 0> 0.000 81.5
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.002 70.6
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.003 326.1
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.004 230.6
KCl (mp-23193) <1 0 0> <1 0 0> 0.006 40.8
KCl (mp-23193) <1 1 0> <1 1 0> 0.007 57.7
KCl (mp-23193) <1 1 1> <1 1 1> 0.007 70.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.008 81.5
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.009 282.4
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.009 70.6
Au (mp-81) <1 1 1> <1 1 1> 0.011 211.8
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.013 282.4
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.015 173.0
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.015 211.8
PbS (mp-21276) <1 0 0> <1 0 0> 0.018 326.1
GaN (mp-804) <0 0 1> <1 0 0> 0.021 285.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.026 163.1
BN (mp-984) <0 0 1> <1 1 1> 0.027 70.6
ZnO (mp-2133) <0 0 1> <1 0 0> 0.035 326.1
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.043 244.6
GaP (mp-2490) <1 1 0> <1 1 0> 0.044 173.0
GaP (mp-2490) <1 1 1> <1 1 1> 0.044 211.8
CdS (mp-672) <0 0 1> <1 1 0> 0.046 230.6
Ag (mp-124) <1 1 1> <1 1 1> 0.054 211.8
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.060 163.1
CsI (mp-614603) <1 1 0> <1 1 0> 0.064 173.0
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.069 244.6
GaN (mp-804) <1 0 0> <1 0 0> 0.072 203.8
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.073 163.1
WS2 (mp-224) <0 0 1> <1 0 0> 0.083 285.4
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.084 285.4
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.095 230.6
AlN (mp-661) <0 0 1> <1 0 0> 0.110 203.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.114 163.1
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.118 173.0
AlN (mp-661) <1 0 0> <1 0 0> 0.120 285.4
AlN (mp-661) <1 0 1> <1 0 0> 0.123 285.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.132 115.3
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.135 288.3
LaF3 (mp-905) <0 0 1> <1 1 0> 0.144 230.6
Te2W (mp-22693) <1 0 1> <1 0 0> 0.151 203.8
Mg (mp-153) <0 0 1> <1 0 0> 0.152 285.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.156 326.1
Te2Mo (mp-602) <1 0 1> <1 1 1> 0.159 282.4
Mg (mp-153) <1 0 0> <1 0 0> 0.161 203.8
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.182 173.0
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.188 81.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
99 77 77 0 0 0
77 99 77 0 0 0
77 77 99 0 0 0
0 0 0 30 0 0
0 0 0 0 30 0
0 0 0 0 0 30
Compliance Tensor Sij (10-12Pa-1)
31.6 -13.8 -13.8 0 0 0
-13.8 31.6 -13.8 0 0 0
-13.8 -13.8 31.6 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 33
Shear Modulus GV
23 GPa
Bulk Modulus KV
84 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
84 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
84 GPa
Elastic Anisotropy
1.34
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrSiPd (mp-8843) 0.3390 0.000 3
SrSiPt (mp-971914) 0.3332 0.000 3
SrGePt (mp-21164) 0.2673 0.000 3
EuGePt (mp-19798) 0.1527 0.000 3
EuPIr (mp-1095517) 0.3719 0.000 3
BaSi2 (mp-7275) 0.0500 0.013 2
SrSi2 (mp-14172) 0.1183 0.003 2
SrSi2 (mp-496) 0.1184 0.003 2
NbSe4 (mp-1078815) 0.7395 0.030 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Si Pt
Final Energy/Atom
-5.4708 eV
Corrected Energy
-65.3661 eV
Uncorrected energy = -65.6501 eV Composition-based energy adjustment (0.071 eV/atom x 4.0 atoms) = 0.2840 eV Corrected energy = -65.3661 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 72640
  • 63555
Submitted by
User remarks:
  • Calcium platinum silicide - I

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)