material

MnCo2Si

ID:

mp-4492

DOI:

10.17188/1208189


Tags: Cobalt manganese silicide (2/1/1) Cobalt manganese silicon (2/1/1)

Material Details

Final Magnetic Moment
5.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.454 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 624141 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 1 0> <1 1 0> 0.000 269.2
MgO (mp-1265) <1 1 1> <1 1 1> 0.001 219.8
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.006 164.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.008 285.6
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.009 164.9
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.018 95.2
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.018 219.8
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.018 158.6
GaSe (mp-1943) <0 0 1> <1 1 1> 0.021 164.9
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.023 134.6
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.024 63.5
Au (mp-81) <1 1 0> <1 1 0> 0.026 269.2
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.027 158.6
InP (mp-20351) <1 0 0> <1 0 0> 0.030 285.6
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.038 63.5
C (mp-66) <1 0 0> <1 0 0> 0.039 63.5
BN (mp-984) <1 0 1> <1 1 0> 0.075 179.5
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.077 31.7
PbS (mp-21276) <1 0 0> <1 0 0> 0.078 285.6
CdS (mp-672) <1 0 0> <1 1 0> 0.097 314.1
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.110 190.4
ZnO (mp-2133) <1 1 1> <1 1 0> 0.111 314.1
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.115 63.5
ZnO (mp-2133) <1 1 0> <1 1 0> 0.134 89.7
Au (mp-81) <1 0 0> <1 0 0> 0.142 158.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.180 219.8
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.186 222.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.188 285.6
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.205 269.2
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.205 158.6
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.215 317.3
C (mp-48) <0 0 1> <1 1 0> 0.242 314.1
GaN (mp-804) <1 0 0> <1 0 0> 0.266 253.8
WS2 (mp-224) <1 1 0> <1 0 0> 0.272 158.6
AlN (mp-661) <0 0 1> <1 0 0> 0.273 317.3
Ag (mp-124) <1 0 0> <1 0 0> 0.275 158.6
WS2 (mp-224) <1 1 1> <1 0 0> 0.293 158.6
Al (mp-134) <1 1 1> <1 0 0> 0.294 222.1
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.311 63.5
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.320 44.9
TePb (mp-19717) <1 1 0> <1 1 0> 0.333 179.5
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.335 44.9
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.338 285.6
TePb (mp-19717) <1 1 1> <1 1 1> 0.339 219.8
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.356 31.7
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.366 222.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.369 158.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.369 158.6
NaCl (mp-22862) <1 0 0> <1 0 0> 0.373 31.7
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.373 285.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
314 172 172 0 0 0
172 314 172 0 0 0
172 172 314 0 0 0
0 0 0 142 0 0
0 0 0 0 142 0
0 0 0 0 0 142
Compliance Tensor Sij (10-12Pa-1)
5.2 -1.8 -1.8 0 0 0
-1.8 5.2 -1.8 0 0 0
-1.8 -1.8 5.2 0 0 0
0 0 0 7.1 0 0
0 0 0 0 7.1 0
0 0 0 0 0 7.1
Shear Modulus GV
113 GPa
Bulk Modulus KV
219 GPa
Shear Modulus GR
101 GPa
Bulk Modulus KR
219 GPa
Shear Modulus GVRH
107 GPa
Bulk Modulus KVRH
219 GPa
Elastic Anisotropy
0.59
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MnAlRh2 (mp-10894) 0.0000 0.000 3
FeCo2Ge (mp-22300) 0.0000 0.000 3
Li2CuSb (mp-15988) 0.0000 0.000 3
ScInCu2 (mp-21067) 0.0000 0.000 3
ZrNi2Sb (mp-19904) 0.0000 0.146 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Mn3Si (mp-20211) 0.0000 0.000 2
NaIn (mp-20628) 0.0000 0.000 2
AlFe3 (mp-2018) 0.0000 0.004 2
AlCu3 (mp-12777) 0.0000 0.025 2
CeCd3 (mp-2863) 0.0000 0.000 2
Mg (mp-110) 0.0000 0.022 1
Fe (mp-13) 0.0000 0.000 1
Nb (mp-75) 0.0000 0.000 1
Li (mp-135) 0.0000 0.005 1
Pu (mp-107) 0.0000 0.546 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Co Si
Final Energy/Atom
-7.6540 eV
Corrected Energy
-30.5448 eV
Uncorrected energy = -30.6158 eV Composition-based energy adjustment (0.071 eV/atom x 1.0 atoms) = 0.0710 eV Corrected energy = -30.5448 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 624144
  • 624157
  • 624143
  • 659021
  • 53007
  • 624141
Submitted by
User remarks:
  • Cobalt manganese silicon (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)