material

ZrNbP

ID:

mp-4500

DOI:

10.17188/1208215


Tags: Zirconium niobium phosphide (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.079 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 75008 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.002 313.8
GaSe (mp-1943) <0 0 1> <0 1 0> 0.008 239.9
KTaO3 (mp-3614) <1 0 0> <0 1 1> 0.008 194.7
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.009 239.9
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.009 239.9
NaCl (mp-22862) <1 0 0> <0 1 1> 0.010 194.7
Ag (mp-124) <1 0 0> <1 0 0> 0.017 172.9
Mg (mp-153) <0 0 1> <0 1 0> 0.022 209.9
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.026 198.9
GaTe (mp-542812) <1 0 0> <0 1 0> 0.032 89.9
AlN (mp-661) <0 0 1> <0 1 0> 0.035 269.8
Al (mp-134) <1 0 0> <0 1 1> 0.035 194.7
YVO4 (mp-19133) <0 0 1> <0 1 1> 0.046 155.8
GaN (mp-804) <1 0 1> <0 0 1> 0.054 248.6
Au (mp-81) <1 0 0> <1 0 0> 0.057 172.9
AlN (mp-661) <1 1 0> <0 1 0> 0.062 269.8
Cu (mp-30) <1 0 0> <0 1 1> 0.064 38.9
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.077 209.9
TiO2 (mp-390) <0 0 1> <0 1 1> 0.078 116.8
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.078 188.3
WS2 (mp-224) <0 0 1> <0 1 0> 0.078 209.9
LiNbO3 (mp-3731) <0 0 1> <1 0 1> 0.086 188.3
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.092 129.9
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.094 223.7
WSe2 (mp-1821) <1 0 0> <1 0 1> 0.095 251.1
AlN (mp-661) <1 0 1> <0 1 1> 0.101 194.7
MoSe2 (mp-1634) <1 0 1> <1 1 0> 0.122 259.9
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.123 223.7
LiTaO3 (mp-3666) <1 1 0> <1 0 1> 0.127 125.5
CsI (mp-614603) <1 1 0> <1 1 0> 0.132 259.9
Mg (mp-153) <1 0 0> <0 1 0> 0.138 269.8
GdScO3 (mp-5690) <1 1 0> <0 1 1> 0.146 194.7
CaCO3 (mp-3953) <1 0 1> <0 1 1> 0.148 272.6
NdGaO3 (mp-3196) <0 1 1> <0 1 0> 0.149 209.9
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.149 223.7
GaP (mp-2490) <1 1 0> <1 1 0> 0.155 129.9
WS2 (mp-224) <1 1 1> <0 1 0> 0.161 239.9
InP (mp-20351) <1 1 0> <0 1 0> 0.165 149.9
CdWO4 (mp-19387) <0 0 1> <1 1 1> 0.178 278.2
YAlO3 (mp-3792) <1 0 1> <0 1 1> 0.185 194.7
MgF2 (mp-1249) <1 0 0> <0 1 1> 0.189 272.6
Mg (mp-153) <1 0 1> <0 0 1> 0.190 248.6
BaTiO3 (mp-5986) <0 0 1> <0 1 1> 0.191 194.7
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.203 129.9
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.210 251.1
CdS (mp-672) <1 1 1> <0 1 1> 0.210 155.8
CdS (mp-672) <1 1 0> <0 0 1> 0.214 49.7
CdS (mp-672) <1 0 0> <1 0 0> 0.221 57.6
Cu (mp-30) <1 1 0> <0 0 1> 0.222 74.6
CdS (mp-672) <0 0 1> <0 0 1> 0.229 198.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
299 85 139 0 0 0
85 320 114 0 0 0
139 114 270 0 0 0
0 0 0 117 0 0
0 0 0 0 126 0
0 0 0 0 0 82
Compliance Tensor Sij (10-12Pa-1)
4.5 -0.4 -2.1 0 0 0
-0.4 3.7 -1.4 0 0 0
-2.1 -1.4 5.4 0 0 0
0 0 0 8.5 0 0
0 0 0 0 7.9 0
0 0 0 0 0 12.1
Shear Modulus GV
102 GPa
Bulk Modulus KV
174 GPa
Shear Modulus GR
97 GPa
Bulk Modulus KR
174 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
174 GPa
Elastic Anisotropy
0.28
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HfSiMo (mp-22258) 0.3062 0.000 3
ZrVP (mp-22302) 0.3656 0.000 3
HfNbP (mp-22637) 0.1346 0.000 3
HfVP (mp-1095442) 0.3056 0.000 3
HfGeMo (mp-1095449) 0.2879 0.000 3
KSr2Cd2Sb3 (mp-866639) 0.7276 0.000 4
US2 (mp-669500) 0.3756 0.000 2
USe2 (mp-20077) 0.4460 0.036 2
PbCl2 (mp-619071) 0.4589 0.023 2
Lu5Ga3 (mp-1094132) 0.4203 0.009 2
V2P (mp-20541) 0.2275 0.000 2
Rb (mp-640416) 0.4481 0.057 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Nb_pv P
Final Energy/Atom
-9.1001 eV
Corrected Energy
-109.2013 eV
-109.2013 eV = -109.2013 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 75008
Submitted by
User remarks:
  • Zirconium niobium phosphide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)