Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.308 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.048 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 218.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 256.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 222.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 256.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 205.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 307.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 290.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 153.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 231.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 153.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 239.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 272.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 205.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 273.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 359.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 307.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 286.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 286.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 85.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 158.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 218.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 136.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 171.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 307.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 153.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 231.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 17.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 119.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 57.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 188.1 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 273.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 17.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 171.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 324.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 237.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 273.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 308.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 256.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 85.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 205.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 324.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 17.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.85 | -0.00 | -0.00 |
-0.00 | 6.85 | -0.00 |
-0.00 | -0.00 | 5.78 |
Dielectric Tensor εij (total) |
||
---|---|---|
24.63 | -0.00 | -0.00 |
-0.00 | 24.63 | -0.00 |
-0.00 | -0.00 | 16.99 |
Polycrystalline dielectric constant
εpoly∞
6.50
|
Polycrystalline dielectric constant
εpoly
22.08
|
Refractive Index n2.55 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Eu2SeO2 (mp-753314) | 0.0479 | 0.044 | 3 |
Tm2SeO2 (mp-754475) | 0.0544 | 0.045 | 3 |
Nd2TeO2 (mp-5459) | 0.0267 | 0.000 | 3 |
Pr2TeO2 (mp-16032) | 0.0135 | 0.000 | 3 |
Sm2TeO2 (mp-16033) | 0.0542 | 0.000 | 3 |
KLiZnS2 (mp-774907) | 0.3354 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.4511 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.4478 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.2788 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.3186 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.6967 | 0.125 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Te O |
Final Energy/Atom-7.6096 eV |
Corrected Energy-39.4525 eV
-39.4525 eV = -38.0479 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|