Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.662 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.022 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BaCO3
Band Gap
4.440 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [160]
Hall
R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 158389 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.005 75.6
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.005 126.0
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.006 201.5
InSb (mp-20012) <1 0 0> <1 1 0> 0.012 88.4
C (mp-48) <0 0 1> <0 0 1> 0.013 100.8
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.013 88.4
CdTe (mp-406) <1 0 0> <1 1 0> 0.013 88.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.016 25.2
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.016 265.1
TePb (mp-19717) <1 1 0> <1 1 1> 0.017 183.8
CdTe (mp-406) <1 1 1> <0 0 1> 0.018 75.6
Ni (mp-23) <1 1 0> <1 1 1> 0.022 275.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.025 75.6
InP (mp-20351) <1 0 0> <1 1 0> 0.028 176.7
MgF2 (mp-1249) <1 1 0> <1 1 1> 0.030 183.8
KP(HO2)2 (mp-23959) <0 1 0> <1 0 1> 0.031 227.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.032 176.3
AlN (mp-661) <0 0 1> <0 0 1> 0.032 25.2
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.037 302.3
ZnO (mp-2133) <1 0 0> <0 0 1> 0.039 226.7
ZrO2 (mp-2858) <1 0 1> <1 0 1> 0.042 170.7
SiC (mp-8062) <1 1 1> <0 0 1> 0.043 100.8
CdTe (mp-406) <1 1 0> <1 1 1> 0.046 183.8
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.046 88.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.047 306.1
Au (mp-81) <1 0 0> <1 1 0> 0.047 88.4
C (mp-66) <1 1 0> <1 0 0> 0.050 255.1
TePb (mp-19717) <1 1 1> <0 0 1> 0.051 75.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.053 25.2
GaN (mp-804) <0 0 1> <0 0 1> 0.053 226.7
InSb (mp-20012) <1 1 0> <1 1 1> 0.054 183.8
SiC (mp-11714) <0 0 1> <0 0 1> 0.058 25.2
Al (mp-134) <1 0 0> <1 0 0> 0.070 306.1
KP(HO2)2 (mp-23959) <0 0 1> <1 0 1> 0.074 227.6
SrTiO3 (mp-4651) <1 0 1> <1 1 0> 0.080 265.1
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.081 327.5
TiO2 (mp-2657) <0 0 1> <1 1 0> 0.084 88.4
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.086 255.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.090 75.6
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.091 302.3
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.095 153.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.103 226.7
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.104 204.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.104 302.3
AlN (mp-661) <1 1 0> <0 0 1> 0.108 302.3
TiO2 (mp-390) <0 0 1> <1 0 0> 0.108 255.1
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.113 204.1
TePb (mp-19717) <1 0 0> <1 1 0> 0.119 88.4
C (mp-48) <1 0 0> <1 0 0> 0.122 153.1
SiC (mp-11714) <1 0 1> <1 0 1> 0.123 227.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
107 38 32 -6 0 0
38 107 32 6 0 0
32 32 41 0 0 0
-6 6 0 18 0 0
0 0 0 0 18 -6
0 0 0 0 -6 34
Compliance Tensor Sij (10-12Pa-1)
12.9 -2.5 -8.0 5.0 0.0 0.0
-2.5 12.9 -8.0 -5.0 0.0 0.0
-8.0 -8.0 36.9 0.0 -0.0 -0.0
5.0 -5.0 0.0 58.3 0.0 0.0
0.0 0.0 -0.0 0.0 58.3 9.9
0.0 0.0 -0.0 0.0 9.9 30.9
Shear Modulus GV
24 GPa
Bulk Modulus KV
51 GPa
Shear Modulus GR
20 GPa
Bulk Modulus KR
39 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
45 GPa
Elastic Anisotropy
1.51
Poisson's Ratio
0.29

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -0.01497 -0.04083
-0.04083 0.04083 0.00000 -0.01498 0.00000 0.00000
0.30619 0.30619 0.44322 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.61964 C/m2
Crystallographic Direction vmax
-0.00000
0.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.05 0.00 0.00
0.00 3.05 0.00
0.00 0.00 2.39
Dielectric Tensor εij (total)
9.51 0.00 0.00
0.00 9.51 0.00
0.00 0.00 6.80
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.83
Polycrystalline dielectric constant εpoly
(total)
8.61
Refractive Index n
1.68
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KNO3 (mp-6920) 0.1515 0.002 3
BaCO3 (mp-34195) 0.2892 0.035 3
KNO3 (mp-36903) 0.2760 0.007 3
CsBeH3 (mp-24341) 0.3070 0.000 3
AgNO3 (mp-8196) 0.2124 0.031 3
Cs2Sr2(CO3)3 (mp-866617) 0.5462 0.001 4
SmH3(CO2)3 (mp-23771) 0.5510 0.117 4
NdH3(CO2)3 (mp-23837) 0.5409 0.113 4
LaH3(CO2)3 (mp-642729) 0.5417 0.083 4
Pb2CO3F2 (mp-555946) 0.4771 0.002 4
Ba2GdC2(O2F)3 (mp-8986) 0.5006 0.000 5
Ba2YC2(O2F)3 (mp-8985) 0.5100 0.000 5
C (mp-569304) 0.5070 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

A new quaternary sulfide, BaLa2MnS5, was prepared by the reaction of CS2 with a mixture of BaCO3, La2O3, and MnO2 at 1323 K. The crystal structure of this compound is tetragonal with space group I4/mc [...]
The structure and composition of a new SO24-stabilized phase of barium carbonate, -BaCO3, have been characterized. Fine crystalline powder of -BaCO3 was prepared from BaCO3 with a few mole% of BaSO [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition BaCO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv C O
Final Energy/Atom
-7.4475 eV
Corrected Energy
-39.2985 eV
Uncorrected energy = -37.2375 eV Composition-based energy adjustment (-0.687 eV/atom x 3.0 atoms) = -2.0610 eV Corrected energy = -39.2985 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 158389
  • 158390
Submitted by
User remarks:
  • Witherite
  • Barium carbonate - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)