material

SrHfO3

ID:

mp-4673

DOI:

10.17188/1208330


Tags: Strontium hafnate Strontium hafnate - HT Strontium hafnate - hypothetical, unlikely

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.818 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.004 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.49 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SrHfO3
Band Gap
3.955 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 89384 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 0 0> <0 1 0> 0.015 269.3
CeO2 (mp-20194) <1 0 0> <0 1 0> 0.015 269.3
LiGaO2 (mp-5854) <1 0 1> <0 1 0> 0.038 134.7
Ni (mp-23) <1 1 0> <0 1 1> 0.038 190.9
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.052 269.3
GaN (mp-804) <0 0 1> <1 1 1> 0.052 117.2
MgAl2O4 (mp-3536) <1 0 0> <0 1 0> 0.067 67.3
LiF (mp-1138) <1 0 0> <0 1 0> 0.079 67.3
C (mp-66) <1 1 0> <0 1 1> 0.106 286.4
Ga2O3 (mp-886) <1 0 0> <0 1 1> 0.121 286.4
MgAl2O4 (mp-3536) <1 1 0> <0 1 1> 0.127 95.5
LiF (mp-1138) <1 1 0> <0 1 1> 0.144 95.5
Ge (mp-32) <1 0 0> <0 1 0> 0.149 67.3
GaP (mp-2490) <1 0 0> <0 1 0> 0.151 269.3
Mg (mp-153) <1 1 1> <0 1 0> 0.152 269.3
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.168 117.2
LiF (mp-1138) <1 1 1> <1 1 1> 0.189 117.2
LiAlO2 (mp-3427) <0 0 1> <0 1 0> 0.207 134.7
CaF2 (mp-2741) <1 0 0> <0 1 0> 0.234 269.3
Ge (mp-32) <1 1 0> <0 1 1> 0.235 95.5
GaAs (mp-2534) <1 0 0> <0 1 0> 0.251 67.3
Ga2O3 (mp-886) <0 1 0> <0 1 1> 0.252 286.4
TeO2 (mp-2125) <1 0 0> <0 1 1> 0.266 286.4
Ag (mp-124) <1 0 0> <1 0 0> 0.274 68.1
SiO2 (mp-6930) <1 0 1> <0 1 1> 0.308 286.4
Al (mp-134) <1 0 0> <1 0 0> 0.316 272.2
ZnSe (mp-1190) <1 0 0> <0 1 0> 0.328 67.3
GaAs (mp-2534) <1 1 0> <0 1 1> 0.360 95.5
Mg (mp-153) <1 0 1> <1 0 0> 0.372 204.2
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.389 270.7
Mg (mp-153) <1 0 0> <0 1 1> 0.408 286.4
Ag (mp-124) <1 1 0> <1 1 0> 0.409 95.7
GdScO3 (mp-5690) <0 1 0> <0 1 0> 0.420 134.7
InSb (mp-20012) <1 1 0> <0 1 1> 0.425 190.9
Ag (mp-124) <1 1 1> <1 1 1> 0.428 117.2
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.439 134.7
Al2O3 (mp-1143) <1 0 0> <0 1 1> 0.443 190.9
ZnSe (mp-1190) <1 1 0> <0 1 1> 0.451 95.5
Au (mp-81) <1 0 0> <1 0 0> 0.460 68.1
CdTe (mp-406) <1 1 0> <0 1 1> 0.469 190.9
Ga2O3 (mp-886) <1 1 0> <0 1 1> 0.535 286.4
TeO2 (mp-2125) <1 1 0> <0 1 0> 0.538 202.0
GaN (mp-804) <1 1 1> <0 1 0> 0.570 269.3
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.593 117.2
GdScO3 (mp-5690) <1 0 0> <0 1 1> 0.630 95.5
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.645 134.7
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.689 269.3
CdWO4 (mp-19387) <0 1 0> <0 1 0> 0.731 134.7
NdGaO3 (mp-3196) <0 0 1> <0 1 0> 0.736 269.3
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.808 134.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
272 128 69 0 0 0
128 284 78 0 0 0
69 78 288 0 0 0
0 0 0 69 0 0
0 0 0 0 87 0
0 0 0 0 0 93
Compliance Tensor Sij (10-12Pa-1)
4.8 -2.0 -0.6 0.0 0 0
-2.0 4.6 -0.8 -0.0 0 0
-0.6 -0.8 3.8 0.0 0 0
0.0 -0.0 0.0 14.6 0 0
0 0 0 0 11.5 0
0 0 0 0 0 10.8
Shear Modulus GV
88 GPa
Bulk Modulus KV
155 GPa
Shear Modulus GR
85 GPa
Bulk Modulus KR
154 GPa
Shear Modulus GVRH
86 GPa
Bulk Modulus KVRH
155 GPa
Elastic Anisotropy
0.17
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrZrO3 (mp-3626) 0.2265 0.008 3
KMgCl3 (mp-27865) 0.3407 0.003 3
CsPbBr3 (mp-567629) 0.3473 0.001 3
NaTaO3 (mp-4699) 0.2209 0.001 3
NaNbO3 (mp-4748) 0.2404 0.024 3
Sr2MnMoO6 (mp-705116) 0.3467 0.006 4
SrCa3Mn4O12 (mp-1094044) 0.5118 0.060 4
Sr3Ca(FeO3)4 (mp-1094055) 0.4459 0.013 4
Sr2LuIrO6 (mp-561683) 0.5224 0.000 4
CaLaMn2O6 (mvc-11813) 0.4969 0.105 4
Na3LaTi2Nb2O12 (mp-695512) 0.3557 0.017 5
Sr8Nd2Fe5(MoO6)5 (mp-744876) 0.5004 0.011 5
CaNd2Ti2Mn2O12 (mvc-11950) 0.5026 0.182 5
CaLa2Ti2Mn2O12 (mvc-14929) 0.4960 0.132 5
Na3SrTiNb3O12 (mp-677431) 0.4682 0.029 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Hf_pv O
Final Energy/Atom
-8.6944 eV
Corrected Energy
-182.1323 eV
Uncorrected energy = -173.8883 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Corrected energy = -182.1323 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 161596
  • 89384
  • 164622
Submitted by
User remarks:
  • Strontium hafnate - hypothetical, unlikely

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)