material

Zn(CrSe2)2

ID:

mp-4697

DOI:

10.17188/1208343


Tags: Zinc dichromium selenide Zinc dichromium tetraselenide Dichromium zinc selenide Zinc chromium selenide (1/2/4)

Material Details

Final Magnetic Moment
5.995 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.595 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.049 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 53217 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <1 0 0> 0.000 224.9
C (mp-48) <0 0 1> <1 1 1> 0.001 194.8
Au (mp-81) <1 0 0> <1 0 0> 0.017 224.9
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.025 112.5
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.038 194.8
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.046 194.8
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.061 224.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.063 112.5
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.065 159.0
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.066 194.8
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.070 194.8
YAlO3 (mp-3792) <1 0 0> <1 1 0> 0.133 159.0
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.146 112.5
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.166 112.5
TiO2 (mp-390) <1 0 1> <1 1 0> 0.167 159.0
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.190 224.9
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.195 112.5
InAs (mp-20305) <1 1 0> <1 1 0> 0.200 159.0
InAs (mp-20305) <1 1 1> <1 1 1> 0.203 194.8
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.222 159.0
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.223 159.0
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.226 194.8
AlN (mp-661) <1 1 1> <1 0 0> 0.243 112.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.243 224.9
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.255 112.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.271 224.9
GaTe (mp-542812) <1 0 0> <1 0 0> 0.280 224.9
SiC (mp-7631) <1 1 0> <1 1 0> 0.300 159.0
CdSe (mp-2691) <1 1 0> <1 1 0> 0.471 159.0
CdSe (mp-2691) <1 1 1> <1 1 1> 0.478 194.8
Te2W (mp-22693) <0 1 0> <1 1 0> 0.513 159.0
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.566 159.0
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.585 224.9
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 1.652 112.5
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 1.727 159.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 1.752 194.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
100 53 53 0 0 0
53 100 53 0 0 0
53 53 100 0 0 0
0 0 0 38 0 0
0 0 0 0 38 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
15.7 -5.4 -5.4 0 0 0
-5.4 15.7 -5.4 0 0 0
-5.4 -5.4 15.7 0 0 0
0 0 0 26.7 0 0
0 0 0 0 26.7 0
0 0 0 0 0 26.7
Shear Modulus GV
32 GPa
Bulk Modulus KV
69 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
69 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
69 GPa
Elastic Anisotropy
0.26
Poisson's Ratio
0.30

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -5.515 21.329 4.100 6.024
pack_evans_james -5.515 21.330 0.454 3.343
vinet -5.515 21.316 4.169 5.122
tait -5.515 21.315 0.460 5.481
birch_euler -5.515 21.327 0.514 0.353
pourier_tarantola -5.516 21.309 0.079 2.414
birch_lagrange -5.521 21.316 0.293 6.082
murnaghan -5.514 21.352 0.444 3.210
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn(RhO2)2 (mp-5146) 0.0017 0.000 3
In2HgS4 (mp-22356) 0.0027 0.000 3
Li2MnF4 (mp-778547) 0.0021 0.054 3
Zn(CrSe2)2 (mvc-11651) 0.0000 0.000 3
Zn(CrS2)2 (mp-4194) 0.0030 0.000 3
Li2V3CrO8 (mp-853131) 0.0825 0.032 4
Li2TiFe3O8 (mp-850231) 0.0792 0.045 4
Li2Fe3CuO8 (mp-772689) 0.0732 0.046 4
Li2V3CoO8 (mp-765546) 0.0667 0.223 4
Li2Ti3CrO8 (mp-771759) 0.0864 0.005 4
Hf3N4 (mp-755988) 0.1153 0.016 2
Zr3N4 (mp-754381) 0.1171 0.035 2
In3S4 (mp-556597) 0.0412 0.042 2
Sn3N4 (mp-16031) 0.0634 0.000 2
Ge3N4 (mp-476) 0.1004 0.109 2
Li4Cr2Fe3Co3O16 (mp-775698) 0.3797 0.897 5
Li14Mn22Cr3Cu3O56 (mp-735790) 0.3513 0.014 5
Li4Mn3Cr3(CuO8)2 (mp-765456) 0.3512 0.069 5
Li4Cr3Cu3(SbO8)2 (mp-783908) 0.3772 0.035 5
Li4Cr3Fe3(SbO8)2 (mp-771925) 0.3789 6.495 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Cr_pv Se
Final Energy/Atom
-5.5305 eV
Corrected Energy
-81.2032 eV
Uncorrected energy = -77.4272 eV Composition-based energy adjustment (-0.472 eV/atom x 8.0 atoms) = -3.7760 eV Corrected energy = -81.2032 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 604584
  • 174098
  • 53217
  • 626745
  • 626749
  • 150966
  • 626755
  • 626758
  • 626757
  • 626748
  • 626760
  • 626751
  • 626753
  • 626746
Submitted by
User remarks:
  • Zinc chromium selenide (1/2/4)