material

ZrSiO4

ID:

mp-4820

DOI:

10.17188/1208424


Tags: High pressure experimental phase Zircon (Dy-doped) Zircon Zirconium silicate Zirconium silicate - V-doped

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.569 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.458 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I41/amd [141]
Hall
I 4bw 2bw 1bw
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 9582 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbS (mp-21276) <1 0 0> <0 0 1> 0.001 180.0
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.030 229.2
MgO (mp-1265) <1 0 0> <0 0 1> 0.033 90.0
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.036 225.0
Te2W (mp-22693) <1 0 0> <1 1 1> 0.043 291.4
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.065 283.6
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.075 242.2
AlN (mp-661) <1 0 1> <1 0 0> 0.076 283.6
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.088 225.0
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.094 242.2
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.099 283.6
Cu (mp-30) <1 0 0> <0 0 1> 0.105 225.0
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.108 270.0
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.108 202.6
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.110 202.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.110 202.6
Mg (mp-153) <0 0 1> <1 0 0> 0.111 202.6
Al (mp-134) <1 0 0> <1 0 1> 0.131 242.2
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.136 242.2
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.137 315.0
MgF2 (mp-1249) <1 1 1> <1 0 1> 0.141 60.6
InP (mp-20351) <1 0 0> <0 0 1> 0.154 180.0
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.158 286.5
SiC (mp-11714) <0 0 1> <1 0 1> 0.163 181.7
InSb (mp-20012) <1 1 0> <0 0 1> 0.167 315.0
SiC (mp-7631) <0 0 1> <1 0 1> 0.167 181.7
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.178 121.6
Ni (mp-23) <1 0 0> <0 0 1> 0.179 225.0
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.189 202.6
PbS (mp-21276) <1 1 0> <1 0 0> 0.190 202.6
CdTe (mp-406) <1 1 0> <0 0 1> 0.191 315.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.206 315.0
C (mp-48) <0 0 1> <1 0 0> 0.233 202.6
TePb (mp-19717) <1 1 1> <0 0 1> 0.243 225.0
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.251 225.0
InP (mp-20351) <1 1 0> <1 0 0> 0.260 202.6
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.273 270.0
MgO (mp-1265) <1 1 0> <1 0 0> 0.277 202.6
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.299 302.8
GaSe (mp-1943) <0 0 1> <1 0 0> 0.299 202.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.305 225.0
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.322 45.0
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.354 202.6
Cu (mp-30) <1 1 0> <1 0 0> 0.371 243.1
InSb (mp-20012) <1 0 0> <0 0 1> 0.371 45.0
C (mp-66) <1 0 0> <0 0 1> 0.378 225.0
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.401 315.0
CdTe (mp-406) <1 0 0> <0 0 1> 0.413 45.0
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.419 225.0
GaN (mp-804) <0 0 1> <1 0 0> 0.424 202.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
439 142 142 0 0 0
142 372 57 0 0 0
142 57 372 0 0 0
0 0 0 45 0 0
0 0 0 0 98 0
0 0 0 0 0 98
Compliance Tensor Sij (10-12Pa-1)
2.9 -1 -1 0 0 0
-1 3.1 -0.1 0 0 0
-1 -0.1 3.1 0 0 0
0 0 0 22.2 0 0
0 0 0 0 10.2 0
0 0 0 0 0 10.2
Shear Modulus GV
104 GPa
Bulk Modulus KV
207 GPa
Shear Modulus GR
87 GPa
Bulk Modulus KR
200 GPa
Shear Modulus GVRH
96 GPa
Bulk Modulus KVRH
203 GPa
Elastic Anisotropy
1.02
Poisson's Ratio
0.30

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.38 0.00 0.00
0.00 4.12 -0.00
0.00 -0.00 4.12
Dielectric Tensor εij (total)
12.41 0.00 0.00
0.00 13.28 -0.00
0.00 -0.00 13.28
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.21
Polycrystalline dielectric constant εpoly
(total)
12.99
Refractive Index n
2.05
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LuAsO4 (mp-7644) 0.0408 0.000 3
ErAsO4 (mp-772156) 0.0688 0.000 3
TmAsO4 (mp-771977) 0.0562 0.000 3
HfSiO4 (mp-4609) 0.0674 0.000 3
ThGeO4 (mp-4790) 0.0361 0.000 3
CaU(PO4)2 (mp-9360) 0.6080 0.000 4
Ho2SiSO4 (mp-17366) 0.6242 0.019 4
Er2SiSO4 (mp-555990) 0.6104 0.020 4
Ca2AsClO4 (mp-560595) 0.6197 0.000 4
Li2CaHfF8 (mp-16577) 0.6359 0.000 4
TlCl2 (mp-27205) 0.6653 0.000 2
TlBr2 (mp-27398) 0.5459 0.000 2
InI2 (mp-29312) 0.5505 0.000 2
InBr2 (mp-568108) 0.5788 0.000 2
GaCl2 (mp-568848) 0.6183 0.000 2
DyZr9Si9PO40 (mp-686636) 0.4108 0.011 5
YZr5Si5PO24 (mp-532768) 0.4467 0.014 5
KCaNd(PO4)2 (mp-676934) 0.6042 0.000 5
YbZr7Si7PO32 (mp-690946) 0.4597 0.019 5
ErZr11Si11PO48 (mp-690951) 0.3809 0.008 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Si O
Final Energy/Atom
-8.7282 eV
Corrected Energy
-110.2348 eV
Uncorrected energy = -104.7388 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Corrected energy = -110.2348 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 69644
  • 43308
  • 96090
  • 71945
  • 15759
  • 9582
  • 96731
  • 100243
  • 100248
  • 69643
  • 31130
  • 100240
  • 31101
  • 69645
  • 45520
  • 100241
  • 100247
  • 95249
  • 71942
  • 187193
  • 187194
  • 187589
  • 96732
  • 100244
  • 100242
  • 100239
  • 92740
  • 71943
  • 71944
  • 96733
  • 96734
  • 158108
  • 92741
Submitted by
User remarks:
  • Zircon
  • Zirconium silicate - V-doped

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)