material

CuSe

ID:

mp-488

DOI:

10.17188/1208461


Tags: High pressure experimental phase Copper selenide - alpha Copper selenide - gamma Copper selenide - HT Copper selenide (1/1) - subcell Copper selenide Klockmannite

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.123 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.80 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CuSe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 82331 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TePb (mp-19717) <1 1 1> <0 0 1> 0.000 224.0
LaF3 (mp-905) <0 0 1> <0 0 1> 0.000 182.0
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.000 126.0
C (mp-66) <1 1 1> <0 0 1> 0.002 266.0
NaCl (mp-22862) <1 1 1> <0 0 1> 0.002 56.0
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.005 266.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.005 168.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.005 168.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.006 182.0
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.006 112.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.009 266.0
InAs (mp-20305) <1 1 1> <0 0 1> 0.014 266.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.017 266.0
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.019 84.0
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.021 70.3
Ni (mp-23) <1 0 0> <0 0 1> 0.026 98.0
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.027 210.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.032 266.0
Mg (mp-153) <0 0 1> <0 0 1> 0.032 168.0
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.034 126.0
BN (mp-984) <1 0 0> <0 0 1> 0.038 252.0
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.044 140.6
BN (mp-984) <0 0 1> <0 0 1> 0.045 168.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.051 182.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.058 266.0
CdS (mp-672) <0 0 1> <0 0 1> 0.064 182.0
BN (mp-984) <1 1 0> <0 0 1> 0.068 266.0
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.069 322.0
Ni (mp-23) <1 1 0> <0 0 1> 0.070 70.0
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.072 243.5
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.073 126.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.074 126.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.077 182.0
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.078 224.0
AlN (mp-661) <1 0 0> <0 0 1> 0.079 140.0
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.079 182.0
GaN (mp-804) <1 1 0> <0 0 1> 0.080 294.0
GaN (mp-804) <1 0 0> <0 0 1> 0.088 350.0
TiO2 (mp-390) <1 1 1> <0 0 1> 0.088 322.0
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.089 238.0
LiF (mp-1138) <1 0 0> <0 0 1> 0.096 84.0
MgAl2O4 (mp-3536) <1 1 0> <0 0 1> 0.098 280.0
InP (mp-20351) <1 1 1> <0 0 1> 0.101 182.0
BN (mp-984) <1 1 1> <0 0 1> 0.103 308.0
GaN (mp-804) <0 0 1> <0 0 1> 0.103 168.0
NaCl (mp-22862) <1 0 0> <0 0 1> 0.105 224.0
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.105 224.0
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.119 140.6
MgO (mp-1265) <1 0 0> <0 0 1> 0.120 294.0
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.124 294.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
109 80 25 0 0 0
80 109 25 0 0 0
25 25 117 0 0 0
0 0 0 6 0 0
0 0 0 0 6 0
0 0 0 0 0 14
Compliance Tensor Sij (10-12Pa-1)
20.1 -14.5 -1.2 0.0 0.0 -0.0
-14.5 20.1 -1.2 -0.0 0.0 -0.0
-1.2 -1.2 9.0 0.0 -0.0 0.0
-0.0 0.0 0.0 168.2 -0.0 0.0
-0.0 0.0 -0.0 -0.0 168.2 0.0
-0.0 -0.0 0.0 -0.0 -0.0 69.3
Shear Modulus GV
19 GPa
Bulk Modulus KV
66 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
65 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
65 GPa
Elastic Anisotropy
4.39
Poisson's Ratio
0.40

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CuS (mp-504) 0.1990 0.001 2
CuSe (mp-571486) 0.3591 0.000 2
CuS (mp-555599) 0.3307 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

In a typical experiment, a CuSe nanosheet was synthesized through a hot-injection method. To avoid the use of a toxic, pyrophoric, and expensive alkyl phosphine, Se powder was dissolved in a mixture o [...]
Herein, copper selenide nanoparticles (NPs) have been successfully prepared via a novel galvanic route with copper foil reacting with Na2SeSO3 in pH 7.4 aqueous solution. With copper foil as anode, hi [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition CuSe.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv Se
Final Energy/Atom
-3.9202 eV
Corrected Energy
-49.8742 eV
Uncorrected energy = -47.0422 eV Composition-based energy adjustment (-0.472 eV/atom x 6.0 atoms) = -2.8320 eV Corrected energy = -49.8742 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 94677
  • 94673
  • 94678
  • 94681
  • 94674
  • 94679
  • 76960
  • 94672
  • 629029
  • 94680
  • 94670
  • 94676
  • 94675
  • 94671
  • 94683
  • 94682
  • 94684
  • 82331
  • 240
Submitted by
User remarks:
  • Klockmannite
  • Copper selenide - gamma
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)