Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.288 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.66 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.193 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 28749 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.002 164.5
GaAs (mp-2534) <1 0 0> <0 0 1> 0.010 164.5
KCl (mp-23193) <1 0 0> <0 0 1> 0.014 41.1
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.018 246.8
GaN (mp-804) <0 0 1> <0 0 1> 0.021 287.9
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.023 164.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.025 329.1
Al (mp-134) <1 0 0> <0 0 1> 0.032 82.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.036 164.5
SiC (mp-8062) <1 0 0> <0 0 1> 0.037 329.1
Ge (mp-32) <1 0 0> <0 0 1> 0.038 164.5
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.038 316.7
Ni (mp-23) <1 1 1> <1 0 0> 0.040 316.7
C (mp-66) <1 0 0> <0 0 1> 0.040 164.5
BN (mp-984) <0 0 1> <1 1 0> 0.046 223.9
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.046 119.3
Te2W (mp-22693) <0 0 1> <1 0 1> 0.052 89.2
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.069 82.3
LiF (mp-1138) <1 0 0> <0 0 1> 0.079 82.3
GaTe (mp-542812) <0 0 1> <1 1 0> 0.082 223.9
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.083 316.7
PbS (mp-21276) <1 0 0> <0 0 1> 0.091 329.1
Ni (mp-23) <1 1 0> <0 0 1> 0.092 329.1
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.097 238.6
NaCl (mp-22862) <1 0 0> <0 0 1> 0.107 164.5
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.108 237.5
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.111 119.3
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.115 237.5
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.115 205.7
Cu (mp-30) <1 0 0> <0 0 1> 0.134 205.7
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.135 178.4
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.145 164.5
CdS (mp-672) <1 1 1> <0 0 1> 0.153 205.7
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.159 158.4
GaN (mp-804) <1 0 0> <0 0 1> 0.178 205.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.190 329.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.191 329.1
C (mp-48) <0 0 1> <0 0 1> 0.199 205.7
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.200 112.0
Au (mp-81) <1 0 0> <1 0 0> 0.204 158.4
Ni (mp-23) <1 0 0> <1 0 0> 0.205 158.4
AlN (mp-661) <0 0 1> <0 0 1> 0.217 205.7
WS2 (mp-224) <1 0 0> <1 0 1> 0.219 89.2
AlN (mp-661) <1 0 1> <0 0 1> 0.220 287.9
GaTe (mp-542812) <1 0 -1> <1 1 0> 0.221 223.9
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.235 267.7
Cu (mp-30) <1 1 0> <1 1 0> 0.243 112.0
AlN (mp-661) <1 0 0> <0 0 1> 0.254 287.9
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.260 316.7
Ag (mp-124) <1 0 0> <1 0 0> 0.263 158.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
57 33 34 0 0 0
33 57 34 0 0 0
34 34 54 0 0 0
0 0 0 22 0 0
0 0 0 0 22 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
31.6 -10.2 -13.5 0 0 0
-10.2 31.6 -13.5 0 0 0
-13.5 -13.5 35.7 0 0 0
0 0 0 44.5 0 0
0 0 0 0 44.5 0
0 0 0 0 0 44.1
Shear Modulus GV
18 GPa
Bulk Modulus KV
41 GPa
Shear Modulus GR
16 GPa
Bulk Modulus KR
41 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
41 GPa
Elastic Anisotropy
0.65
Poisson's Ratio
0.32

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.01393 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.01393 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.13848
Piezoelectric Modulus ‖eijmax
0.13848 C/m2
Crystallographic Direction vmax
0.00000
-0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
12.57 0.00 0.00
0.00 12.57 0.00
0.00 0.00 13.01
Dielectric Tensor εij (total)
15.07 0.00 0.00
0.00 15.07 0.00
0.00 0.00 15.86
Polycrystalline dielectric constant εpoly
(electronic contribution)
12.72
Polycrystalline dielectric constant εpoly
(total)
15.33
Refractive Index n
3.57
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnSiAs2 (mp-3595) 0.0486 0.000 3
BeSiAs2 (mp-1009087) 0.0537 0.000 3
ZnSiP2 (mp-4763) 0.0181 0.000 3
AlAgTe2 (mp-14092) 0.0529 0.000 3
LiGaTe2 (mp-5048) 0.0522 0.000 3
MnAg2GeTe4 (mp-1025568) 0.0838 0.000 4
MnCu2SnS4 (mp-986979) 0.0972 0.000 4
ZnCu2GeTe4 (mp-1078420) 0.0811 0.005 4
ZnCu2GeSe4 (mp-10824) 0.0887 0.004 4
ZnCu2GeTe4 (mp-12854) 0.0726 0.005 4
BeP2 (mp-27148) 0.0899 0.000 2
Si7Ge (mp-1094056) 0.1326 0.006 2
ZnTe (mp-571195) 0.1275 0.004 2
BC7 (mp-1095030) 0.1139 0.276 2
SiGe (mp-1096549) 0.0979 0.066 2
Si (mp-149) 0.1653 0.000 1
Sn (mp-117) 0.1653 0.000 1
C (mp-66) 0.1653 0.136 1
Ge (mp-32) 0.1653 0.000 1
Se (mp-12771) 0.1653 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ga_d Ag Te
Final Energy/Atom
-3.3251 eV
Corrected Energy
-26.6010 eV
-26.6010 eV = -26.6010 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 605236
  • 605232
  • 28749
  • 71007
  • 605234
  • 156128
  • 605230
Submitted by
User remarks:
  • Silver gallium telluride