material

Y2MgCu2

ID:

mp-4901

DOI:

10.17188/1208477


Tags: Yttrium copper magnesium (2/2/1) Ytterbium copper magnesium (2/2/1)

Material Details

Final Magnetic Moment
0.413 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.237 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.04 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mbm [127]
Hall
-P 4 2ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 411711 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 0 0> <0 0 1> 0.004 236.2
DyScO3 (mp-31120) <0 1 1> <1 1 1> 0.008 213.9
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.010 254.3
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.015 197.8
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.015 282.5
Si (mp-149) <1 1 1> <1 0 0> 0.016 310.8
CeO2 (mp-20194) <1 1 1> <1 0 0> 0.016 310.8
Al (mp-134) <1 1 0> <1 0 0> 0.024 254.3
Si (mp-149) <1 1 0> <1 0 0> 0.024 84.8
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.025 84.8
LiF (mp-1138) <1 0 0> <1 1 0> 0.027 199.8
Ge (mp-32) <1 0 0> <1 1 0> 0.027 199.8
MgAl2O4 (mp-3536) <1 0 0> <1 1 0> 0.029 199.8
CdS (mp-672) <0 0 1> <1 0 0> 0.030 169.5
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.031 254.3
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.033 327.3
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.033 327.3
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.037 279.7
Ni (mp-23) <1 1 0> <1 0 1> 0.038 261.9
SiC (mp-7631) <1 0 0> <0 0 1> 0.038 236.2
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.038 254.3
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.038 310.8
TiO2 (mp-390) <1 0 0> <0 0 1> 0.039 295.3
TbScO3 (mp-31119) <0 1 1> <1 1 1> 0.042 213.9
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.044 279.7
GaAs (mp-2534) <1 0 0> <1 1 0> 0.045 199.8
SiC (mp-7631) <1 0 1> <0 0 1> 0.047 236.2
Mg (mp-153) <1 1 1> <1 1 0> 0.054 119.9
Fe2O3 (mp-24972) <1 0 1> <1 0 0> 0.057 226.0
CaCO3 (mp-3953) <1 0 0> <1 0 1> 0.060 261.9
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.060 226.0
ZnSe (mp-1190) <1 0 0> <1 1 0> 0.064 199.8
SiC (mp-8062) <1 1 1> <1 1 0> 0.067 199.8
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.070 59.1
SiC (mp-7631) <0 0 1> <1 1 0> 0.071 199.8
BN (mp-984) <1 1 1> <0 0 1> 0.071 236.2
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.072 254.3
BaTiO3 (mp-5986) <1 1 1> <1 0 1> 0.072 261.9
SiC (mp-11714) <0 0 1> <1 1 0> 0.073 199.8
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.073 130.9
Si (mp-149) <1 0 0> <0 0 1> 0.075 59.1
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.076 84.8
GaP (mp-2490) <1 1 0> <1 0 0> 0.083 84.8
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.084 295.3
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.088 279.7
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.090 169.5
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.092 254.3
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.094 254.3
Te2W (mp-22693) <1 1 0> <1 0 0> 0.097 113.0
GaP (mp-2490) <1 1 1> <1 0 0> 0.101 310.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
83 51 51 0 0 0
51 78 57 0 0 0
51 57 78 0 0 0
0 0 0 20 0 0
0 0 0 0 21 0
0 0 0 0 0 21
Compliance Tensor Sij (10-12Pa-1)
22.5 -8.5 -8.5 0 0 0
-8.5 30 -16.2 0 0 0
-8.5 -16.2 30 0 0 0
0 0 0 50.5 0 0
0 0 0 0 47.9 0
0 0 0 0 0 47.9
Shear Modulus GV
18 GPa
Bulk Modulus KV
62 GPa
Shear Modulus GR
17 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
62 GPa
Elastic Anisotropy
0.32
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nd2MgCu2 (mp-16638) 0.1022 0.000 3
Sc2InNi2 (mp-13416) 0.0903 0.000 3
Tm2InCu2 (mp-1078916) 0.0872 0.000 3
Y2InCu2 (mp-1079508) 0.0157 0.000 3
Lu2InNi2 (mp-1079510) 0.1160 0.019 3
Zr3Ga2 (mp-30684) 0.3636 0.000 2
Y3Au2 (mp-1080493) 0.4319 0.032 2
Ta3Ga2 (mp-16756) 0.4382 0.000 2
Nb3Ga2 (mp-11393) 0.4292 0.000 2
Gd3Pd2 (mp-22077) 0.4623 0.014 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Mg_pv Cu_pv
Final Energy/Atom
-4.7824 eV
Corrected Energy
-47.8245 eV
Uncorrected energy = -47.8245 eV Corrected energy = -47.8245 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 411711
  • 419472
Submitted by
User remarks:
  • Ytterbium copper magnesium (2/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)