material

ScCo3B2

ID:

mp-4938

DOI:

10.17188/1208500


Tags: Cobalt scandium boride (3/1/2) Sacandium cobalt boride (1/3/2)

Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.546 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.55 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 44179 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 1 1> <0 0 1> 0.001 268.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.009 268.9
C (mp-48) <1 0 1> <1 0 0> 0.011 160.3
WS2 (mp-224) <0 0 1> <0 0 1> 0.022 62.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.023 62.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.023 268.9
TiO2 (mp-390) <1 1 0> <1 0 0> 0.026 262.2
PbS (mp-21276) <1 1 1> <0 0 1> 0.029 62.0
InP (mp-20351) <1 1 0> <1 1 0> 0.034 50.5
CeO2 (mp-20194) <1 0 0> <1 1 0> 0.046 328.0
C (mp-48) <1 1 1> <1 0 0> 0.049 102.0
Si (mp-149) <1 0 0> <1 1 0> 0.049 328.0
SiC (mp-7631) <1 0 0> <1 0 0> 0.059 233.1
Te2W (mp-22693) <1 0 0> <1 0 0> 0.061 291.4
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.066 218.5
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.071 302.8
InP (mp-20351) <1 1 1> <0 0 1> 0.072 62.0
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.073 160.3
Mg (mp-153) <0 0 1> <0 0 1> 0.074 62.0
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.082 151.4
PbS (mp-21276) <1 1 0> <1 1 0> 0.086 50.5
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.086 277.6
NaCl (mp-22862) <1 1 0> <1 1 0> 0.087 277.6
GaN (mp-804) <0 0 1> <0 0 1> 0.092 62.0
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.093 302.8
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.094 218.5
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.095 58.3
Mg (mp-153) <1 1 0> <1 1 0> 0.100 201.9
Au (mp-81) <1 1 1> <1 1 0> 0.102 151.4
Au (mp-81) <1 0 0> <1 0 0> 0.102 87.4
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.106 160.3
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.108 277.6
Al (mp-134) <1 1 0> <1 0 0> 0.111 160.3
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.113 163.1
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.113 163.1
CdS (mp-672) <0 0 1> <0 0 1> 0.116 62.0
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.127 233.1
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.138 186.1
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.147 227.5
AlN (mp-661) <1 0 1> <1 1 0> 0.158 176.6
Ag (mp-124) <1 1 1> <1 1 0> 0.159 151.4
Ag (mp-124) <1 0 0> <1 0 0> 0.159 87.4
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.159 201.9
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.163 268.9
NdGaO3 (mp-3196) <1 0 0> <1 1 1> 0.165 130.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.183 144.8
AlN (mp-661) <1 1 1> <1 1 0> 0.185 201.9
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.186 160.3
InAs (mp-20305) <1 1 1> <0 0 1> 0.188 268.9
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.191 227.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
390 107 165 0 0 0
107 390 165 0 0 0
165 165 349 0 0 0
0 0 0 143 0 0
0 0 0 0 143 0
0 0 0 0 0 141
Compliance Tensor Sij (10-12Pa-1)
3.2 -0.3 -1.4 0 0 0
-0.3 3.2 -1.4 0 0 0
-1.4 -1.4 4.2 0 0 0
0 0 0 7 0 0
0 0 0 0 7 0
0 0 0 0 0 7.1
Shear Modulus GV
132 GPa
Bulk Modulus KV
223 GPa
Shear Modulus GR
127 GPa
Bulk Modulus KR
222 GPa
Shear Modulus GVRH
129 GPa
Bulk Modulus KVRH
223 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
DyCo3B2 (mp-20193) 0.0470 0.000 3
HoCo3B2 (mp-5313) 0.0233 0.000 3
ErCo3B2 (mp-5353) 0.0078 0.000 3
TmCo3B2 (mp-5714) 0.0097 0.000 3
LuCo3B2 (mp-15709) 0.0260 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Co B
Final Energy/Atom
-7.3820 eV
Corrected Energy
-44.2920 eV
-44.2920 eV = -44.2920 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 613280
  • 44179
Submitted by
User remarks:
  • Cobalt scandium boride (3/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)