Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.151 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3n [223] |
Hall-P 4n 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 271.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 321.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 171.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 197.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 139.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 271.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 171.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 197.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 123.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 104.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 123.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 197.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 104.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 171.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 296.6 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 214.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 174.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 123.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 173.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 104.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 197.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 299.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 279.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 279.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 123.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 214.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 174.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 197.8 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 299.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 173.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 104.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 321.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 171.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 69.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 148.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 123.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 69.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 139.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 271.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 148.3 |
BN (mp-984) | <0 0 1> | <1 1 1> | 171.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 271.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 370.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 104.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 222.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 69.9 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 139.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 171.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VGe3 (mp-672337) | 0.0000 | 0.357 | 2 |
Ta3Au (mp-569249) | 0.0000 | 0.009 | 2 |
Cr3Ga (mp-1231) | 0.0000 | 0.007 | 2 |
Nb3Sn (mp-1326) | 0.0000 | 0.000 | 2 |
V3Fe (mp-1079399) | 0.0000 | 0.000 | 2 |
Cs (mp-949029) | 0.0000 | 0.047 | 1 |
F2 (mp-21848) | 0.0000 | 0.000 | 1 |
Rb (mp-974620) | 0.0000 | 0.036 | 1 |
Cr (mp-17) | 0.0000 | 0.085 | 1 |
W (mp-11334) | 0.0000 | 0.087 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d Mo_pv |
Final Energy/Atom-9.4398 eV |
Corrected Energy-75.5185 eV
-75.5185 eV = -75.5185 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)