Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.500 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 178.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 142.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 216.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 216.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 216.2 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 176.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 226.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 151.3 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 226.9 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 123.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 226.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 201.7 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 92.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 100.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 160.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 226.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 216.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 160.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 277.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 216.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 160.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 226.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 216.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 176.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 126.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 226.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 249.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 201.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 124.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 303.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 303.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 201.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 160.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 226.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 277.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 160.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 277.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 216.2 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 154.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 267.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 142.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 320.9 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 226.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 17.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 25.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 30.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 89.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 196.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 142.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
100 | 41 | 41 | 0 | 0 | 0 |
41 | 100 | 41 | 0 | 0 | 0 |
41 | 41 | 100 | 0 | 0 | 0 |
0 | 0 | 0 | 31 | 0 | 0 |
0 | 0 | 0 | 0 | 31 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13 | -3.8 | -3.8 | 0 | 0 | 0 |
-3.8 | 13 | -3.8 | 0 | 0 | 0 |
-3.8 | -3.8 | 13 | 0 | 0 | 0 |
0 | 0 | 0 | 32.3 | 0 | 0 |
0 | 0 | 0 | 0 | 32.3 | 0 |
0 | 0 | 0 | 0 | 0 | 32.3 |
Shear Modulus GV31 GPa |
Bulk Modulus KV61 GPa |
Shear Modulus GR31 GPa |
Bulk Modulus KR61 GPa |
Shear Modulus GVRH31 GPa |
Bulk Modulus KVRH61 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
NdPb3 (mp-20601) | 0.0000 | 0.000 | 2 |
PaIr3 (mp-30741) | 0.0000 | 0.000 | 2 |
Np3Sn (mp-571075) | 0.0000 | 0.276 | 2 |
Mg3Sb (mp-1094724) | 0.0000 | 0.070 | 2 |
URh3 (mp-1064001) | 0.0000 | 0.000 | 2 |
H2 (mp-634659) | 0.0000 | 0.000 | 1 |
Mg (mp-1056702) | 0.0000 | 0.014 | 1 |
N2 (mp-1056857) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.001 | 1 |
Pd (mp-1056438) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Ga_d |
Final Energy/Atom-3.9013 eV |
Corrected Energy-15.6050 eV
Uncorrected energy = -15.6050 eV
Corrected energy = -15.6050 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)