Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.127 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.152 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnna [52] |
Hall-P 2a 2bc |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 203.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 136.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 289.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 236.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 184.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 26.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 226.9 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 300.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 289.4 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 251.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 251.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 251.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 201.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 251.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 136.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 184.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 136.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 90.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 43.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 187.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 214.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 236.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 214.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 67.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 201.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 251.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 312.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 271.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 171.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 214.9 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 128.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 251.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 209.8 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 201.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 251.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 289.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 271.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 209.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 85.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 226.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 250.0 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 62.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 136.1 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 312.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 250.0 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 85.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 209.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 226.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 131.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMnF3 (mp-765433) | 0.3662 | 0.029 | 3 |
LiFeO3 (mp-771612) | 0.1645 | 0.140 | 3 |
NaSbO3 (mp-752755) | 0.3610 | 0.052 | 3 |
LiVF3 (mp-777894) | 0.3096 | 0.211 | 3 |
Mn3TeO6 (mp-770690) | 0.3550 | 0.027 | 3 |
Li2SnTeO6 (mp-8673) | 0.1559 | 0.000 | 4 |
Li4Mn3TeO12 (mp-771455) | 0.1634 | 0.068 | 4 |
Li2TiTeO6 (mp-756117) | 0.2252 | 0.000 | 4 |
Li4Fe3TeO12 (mp-772725) | 0.1966 | 0.112 | 4 |
Li4Nb(FeO4)3 (mp-774238) | 0.2649 | 0.137 | 4 |
FeSb3 (mp-971669) | 0.4836 | 0.000 | 2 |
Te2Ir (mp-569322) | 0.4670 | 0.012 | 2 |
Mn2O3 (mp-565203) | 0.4714 | 0.000 | 2 |
Mn2O3 (mp-542877) | 0.4873 | 0.007 | 2 |
Cu2O3 (mp-771359) | 0.4622 | 0.000 | 2 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.4799 | 0.058 | 5 |
Li4Fe2TeWO12 (mp-768021) | 0.3450 | 0.083 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.4160 | 0.081 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.3939 | 0.054 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.4980 | 0.181 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sb O |
Final Energy/Atom-5.8824 eV |
Corrected Energy-126.0745 eV
-126.0745 eV = -117.6470 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)