Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.239 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2SiO4 + SiO2 |
Band Gap4.606 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 50.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 69.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 248.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 248.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 50.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 143.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 151.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 238.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 151.2 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 138.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 201.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 208.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 165.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 190.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 238.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 251.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 165.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 216.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 138.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 238.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 47.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 165.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 143.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 95.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 208.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 238.3 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 208.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 238.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 302.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 194.1 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 251.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 248.9 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 151.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 151.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 201.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 201.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 333.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 333.6 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 248.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 333.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 69.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 50.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 302.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 333.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 143.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 47.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 151.2 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 277.4 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 50.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 238.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg17(SiO3)16 (mp-757674) | 0.3768 | 0.112 | 3 |
YTcN3 (mp-989640) | 0.3819 | 0.021 | 3 |
YReN3 (mp-989628) | 0.3707 | 0.009 | 3 |
CaReN3 (mp-989606) | 0.3917 | 0.000 | 3 |
MgSiO3 (mp-603930) | 0.2666 | 0.008 | 3 |
LiCo(SiO3)2 (mp-767356) | 0.3248 | 0.099 | 4 |
LiFe(SiO3)2 (mp-510708) | 0.3470 | 0.194 | 4 |
LiV(SiO3)2 (mp-19043) | 0.3262 | 0.052 | 4 |
LiCr(SiO3)2 (mp-18727) | 0.3216 | 0.004 | 4 |
LiTi(SiO3)2 (mp-11206) | 0.3164 | 0.052 | 4 |
MoO2 (mvc-6944) | 0.6704 | 0.387 | 2 |
Li2MnV4NiO12 (mp-862462) | 0.3798 | 0.064 | 5 |
Li6ScFe5(SiO3)12 (mp-767482) | 0.3826 | 0.005 | 5 |
Li8ScFe7(SiO3)16 (mp-775203) | 0.3734 | 0.005 | 5 |
Li2MnV4FeO12 (mp-776234) | 0.3675 | 0.064 | 5 |
Li2MnV4NiO12 (mp-868654) | 0.3798 | 0.064 | 5 |
Li4Mn2CrNi3(PO4)6 (mp-775171) | 0.6163 | 0.085 | 6 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.5756 | 0.085 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5828 | 0.080 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5328 | 0.008 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5700 | 0.778 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si O |
Final Energy/Atom-7.1904 eV |
Corrected Energy-304.4711 eV
-304.4711 eV = -287.6161 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)