Final Magnetic Moment1.522 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.574 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrP2O7 + Li4P2O7 + LiPO3 + O2 |
Band Gap0.166 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 251.4 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 160.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 137.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 251.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 167.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 251.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 137.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 137.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.8 |
BN (mp-984) | <1 0 1> | <1 1 1> | 160.7 |
Al (mp-134) | <1 1 0> | <1 0 0> | 137.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 83.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 251.4 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 167.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 167.6 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 251.4 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 137.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 83.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 251.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 167.6 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 137.3 |
C (mp-48) | <1 0 1> | <1 0 1> | 160.7 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 137.3 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 83.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 167.6 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 137.3 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 1> | 160.7 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 251.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 251.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn7Cr12O48 (mp-774029) | 0.6256 | 0.078 | 3 |
Ti7Cr12O48 (mp-853216) | 0.5533 | 0.091 | 3 |
Fe2(WO4)3 (mvc-8014) | 0.5839 | 0.124 | 3 |
Fe2(MoO4)3 (mvc-8023) | 0.5614 | 0.353 | 3 |
Cr3(FeO6)2 (mvc-7922) | 0.5792 | 0.258 | 3 |
Li6V3P8O29 (mp-761509) | 0.1537 | 0.045 | 4 |
Li6V3P8O29 (mp-773963) | 0.1414 | 0.080 | 4 |
Li6V3P8O29 (mp-773637) | 0.1339 | 0.074 | 4 |
Li6V3P8O29 (mp-773531) | 0.1429 | 0.064 | 4 |
Li6V3P8O29 (mp-765212) | 0.1530 | 0.077 | 4 |
Cr19O48 (mp-850874) | 0.5442 | 0.167 | 2 |
Cr19O48 (mp-780521) | 0.5589 | 0.085 | 2 |
Cr8O21 (mp-565489) | 0.7313 | 0.040 | 2 |
Mn2P2H7NO10 (mp-776862) | 0.6770 | 0.224 | 5 |
FeP3H5NO10 (mp-743646) | 0.5547 | 0.084 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.6753 | 0.061 | 5 |
TeP2H16N2O13 (mp-707772) | 0.6528 | 0.045 | 5 |
SnP4H8N2O13 (mp-603633) | 0.6062 | 0.010 | 5 |
Ti2P4H9C2NO16 (mp-709069) | 0.5438 | 0.039 | 6 |
FeBP2H5NO9 (mp-766957) | 0.6685 | 0.100 | 6 |
VBP2H5NO9 (mp-25798) | 0.6077 | 0.000 | 6 |
AlBP2H5NO9 (mp-24757) | 0.6317 | 0.000 | 6 |
NaMgAl3Si8(HO6)4 (mp-1094103) | 0.6747 | 0.025 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.6999 | 0.050 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-6.9394 eV |
Corrected Energy-691.2346 eV
-691.2346 eV = -638.4238 eV (uncorrected energy) - 40.7328 eV (MP Anion Correction) - 12.0780 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)