Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.385 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 |
Band Gap0.053 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 -1> | 162.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 302.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 302.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 181.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 302.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 210.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 302.6 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 105.2 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 210.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 120.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 105.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 181.6 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 210.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 302.6 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 138.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 302.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 248.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 60.5 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 210.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 210.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 302.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 248.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 138.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 210.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 210.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 60.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 241.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 181.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 210.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 181.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 302.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 302.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 181.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 302.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 302.6 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 173.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 181.6 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 302.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 302.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 -1> | 105.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 181.6 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 248.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 302.6 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 105.2 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 124.3 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 124.3 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 210.3 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 248.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 302.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 302.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-851051) | 0.2690 | 0.070 | 3 |
V2(SO4)3 (mp-25724) | 0.4723 | 0.061 | 3 |
CoPO4 (mp-510669) | 0.4043 | 0.086 | 3 |
TiPO4 (mp-25435) | 0.4306 | 0.087 | 3 |
VPO4 (mp-32453) | 0.4842 | 0.027 | 3 |
TiCr(PO4)2 (mp-770565) | 0.3815 | 0.039 | 4 |
Al2P3(HO3)3 (mp-23995) | 0.3794 | 0.006 | 4 |
TiMn(PO4)2 (mp-773171) | 0.3638 | 0.015 | 4 |
Ti2Fe(PO5)2 (mp-565403) | 0.3694 | 0.000 | 4 |
Fe2P3(HO3)3 (mp-25692) | 0.3780 | 0.112 | 4 |
Cr5O12 (mp-19575) | 0.7209 | 0.025 | 2 |
Cr3O8 (mp-557959) | 0.7447 | 0.048 | 2 |
Ti3MnSb2(PO4)6 (mp-775892) | 0.3315 | 0.089 | 5 |
Ti3FeSb2(PO4)6 (mp-776760) | 0.3586 | 0.084 | 5 |
MnV3Sb2(PO4)6 (mp-767358) | 0.3726 | 0.073 | 5 |
Ti3Mn2Fe(PO4)6 (mp-776918) | 0.3705 | 0.012 | 5 |
Ti3Mn2Cu(PO4)6 (mp-777902) | 0.3629 | 0.029 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5662 | 0.065 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.5441 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.5649 | 0.001 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6021 | 0.041 | 6 |
Na2Li4Ti3Al(PO4)6 (mp-769069) | 0.5876 | 0.087 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv P O |
Final Energy/Atom-7.3644 eV |
Corrected Energy-584.1150 eV
-584.1150 eV = -530.2348 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 20.1702 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)