Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.527 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe2(PO4)3 |
Band Gap2.516 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 297.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 108.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 108.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 297.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 297.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 266.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 266.6 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 256.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 216.1 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 266.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 266.6 |
BN (mp-984) | <1 1 0> | <1 0 1> | 133.3 |
BN (mp-984) | <1 1 1> | <1 0 1> | 133.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 209.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 108.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 133.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 297.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 223.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.4 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 133.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 297.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 297.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 216.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 216.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 223.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 297.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 209.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.4 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 108.1 |
C (mp-66) | <1 1 1> | <1 0 1> | 133.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 148.8 |
C (mp-66) | <1 1 0> | <1 0 0> | 108.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 297.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 108.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 148.8 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 148.8 |
PbSe (mp-2201) | <1 1 1> | <1 0 1> | 133.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 148.8 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 1> | 266.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 297.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 297.6 |
CdSe (mp-2691) | <1 1 1> | <1 0 1> | 133.3 |
C (mp-48) | <0 0 1> | <1 0 0> | 216.1 |
C (mp-48) | <1 1 0> | <1 0 1> | 133.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 216.1 |
Au (mp-81) | <1 1 1> | <1 0 1> | 266.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 297.6 |
WSe2 (mp-1821) | <1 1 0> | <1 0 1> | 266.6 |
WSe2 (mp-1821) | <1 1 1> | <1 0 1> | 266.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni2PO5 (mp-769619) | 0.5986 | 0.042 | 3 |
Mn2PO5 (mp-770540) | 0.5663 | 0.018 | 3 |
Fe4(PO4)3 (mp-31780) | 0.5570 | 0.020 | 3 |
Fe2PO5 (mp-24982) | 0.6113 | 0.018 | 3 |
Cr4(PO4)3 (mp-31658) | 0.6026 | 0.034 | 3 |
Li3Mn2(PO4)3 (mp-762864) | 0.2556 | 0.046 | 4 |
Li3Cr2(PO4)3 (mp-31672) | 0.2273 | 0.036 | 4 |
Li3V2(PO4)3 (mp-32530) | 0.1382 | 0.036 | 4 |
Li3V2(PO4)3 (mp-705382) | 0.2648 | 0.036 | 4 |
Li3Fe2(PO4)3 (mp-705422) | 0.2076 | 0.037 | 4 |
Li3MnV(PO4)3 (mp-775639) | 0.2302 | 0.077 | 5 |
Li6MnV3(PO4)6 (mp-764585) | 0.2338 | 0.054 | 5 |
Li4Mn5Cr(PO4)6 (mp-763334) | 0.3187 | 0.067 | 5 |
Li2MnFe2(PO4)3 (mp-767440) | 0.3103 | 0.057 | 5 |
Li6MnFe3(PO4)6 (mp-771062) | 0.3119 | 0.044 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.3617 | 0.081 | 6 |
Li4V3Cr2Co(PO4)6 (mp-771298) | 0.3691 | 0.078 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.3839 | 0.081 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.3655 | 0.099 | 6 |
Li4TiMn2Ni3(PO4)6 (mp-776756) | 0.3666 | 0.069 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.7461 eV |
Corrected Energy-595.2619 eV
-595.2619 eV = -539.6880 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)