Final Magnetic Moment0.156 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.845 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + CuF2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 242.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 63.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 317.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 149.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 80.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 223.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 253.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 242.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 80.9 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 223.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 261.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 190.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 161.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 253.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 253.9 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 298.0 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 149.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 253.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 223.5 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 190.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 317.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 223.5 |
YVO4 (mp-19133) | <1 0 1> | <1 1 -1> | 136.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 63.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 242.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 190.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 242.6 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 190.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 253.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 317.4 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 298.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 317.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 253.9 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 242.6 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 228.6 |
TeO2 (mp-2125) | <1 1 0> | <1 0 -1> | 298.0 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 190.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 190.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 161.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 223.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 298.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 161.7 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 317.4 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 249.7 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 74.5 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 261.5 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 190.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 161.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VAsO4 (mp-761296) | 0.5466 | 0.060 | 3 |
CrPO4 (mp-31707) | 0.4711 | 0.136 | 3 |
Mn7SiO12 (mp-580307) | 0.6136 | 0.336 | 3 |
GaBiO3 (mp-558285) | 0.5451 | 0.002 | 3 |
Mn4(PO4)3 (mp-32010) | 0.6093 | 0.142 | 3 |
MgNiP2O7 (mvc-5642) | 0.5350 | 0.026 | 4 |
NaSbMoO5 (mp-637336) | 0.4155 | 0.032 | 4 |
Li3Bi5(PO4)6 (mp-26835) | 0.5109 | 0.041 | 4 |
LiVPO5 (mp-763302) | 0.4871 | 0.083 | 4 |
Mg2PClO4 (mp-555396) | 0.5143 | 0.016 | 4 |
LiMnPO4F (mp-762683) | 0.6994 | 0.211 | 5 |
LiMn3P2(HO3)4 (mp-763726) | 0.6336 | 0.479 | 5 |
Na2LiVPO6 (mp-763825) | 0.5846 | 0.094 | 5 |
Li2Mn2Co(PO4)3 (mp-763122) | 0.6964 | 0.086 | 5 |
Li3Mn2P2(O4F)2 (mp-763234) | 0.6510 | 0.024 | 5 |
NaLiMnPCO7 (mp-763833) | 0.7132 | 0.062 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv P O F |
Final Energy/Atom-5.8469 eV |
Corrected Energy-198.3381 eV
-198.3381 eV = -187.1015 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)