Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.729 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.685 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 26.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 74.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 79.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 186.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 111.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 319.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 193.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 238.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 26.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 257.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 111.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 182.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 212.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 137.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 238.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 79.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 26.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 106.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 223.2 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 209.1 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 137.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 193.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 345.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 260.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 185.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 212.4 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 128.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 182.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 79.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 128.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 132.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 297.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 223.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 91.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.9 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 257.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 137.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 228.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 193.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 148.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 186.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 185.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 148.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 223.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 278.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 228.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 193.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 111.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.07 | -0.00 | 0.00 |
-0.00 | 3.07 | 0.00 |
0.00 | 0.00 | 2.97 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.64 | -0.00 | 0.00 |
-0.00 | 3.64 | 0.00 |
0.00 | 0.00 | 4.76 |
Polycrystalline dielectric constant
εpoly∞
3.03
|
Polycrystalline dielectric constant
εpoly
4.02
|
Refractive Index n1.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H2CN2 (mp-703527) | 0.7443 | 0.187 | 3 |
UCO5 (mp-555173) | 0.7414 | 0.001 | 3 |
Tl(CO)2 (mp-607841) | 0.6553 | 0.277 | 3 |
Tl2C3O4 (mp-555790) | 0.7350 | 0.164 | 3 |
UCO5 (mp-29761) | 0.7439 | 0.000 | 3 |
C2NClO (mp-1079864) | 0.5380 | 0.351 | 4 |
C2BrNO (mp-1087519) | 0.6658 | 0.375 | 4 |
C2N (mp-2718) | 0.6077 | 0.365 | 2 |
C11F7 (mp-1588) | 0.6073 | 0.366 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: N O |
Final Energy/Atom-6.0342 eV |
Corrected Energy-91.5013 eV
-91.5013 eV = -84.4784 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)