Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.893 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 291.4 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 139.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 54.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 206.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 174.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 229.7 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 159.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 131.3 |
GaAs (mp-2534) | <1 1 0> | <1 -1 1> | 318.9 |
GaAs (mp-2534) | <1 1 1> | <1 -1 -1> | 171.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 318.7 |
GaAs (mp-2534) | <1 0 0> | <1 -1 -1> | 171.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 284.2 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 341.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 131.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 164.1 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 255.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 257.6 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 291.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 191.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 272.4 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 318.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 222.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 174.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 278.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 174.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 284.2 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 1> | 318.9 |
ZnSe (mp-1190) | <1 1 1> | <1 -1 -1> | 171.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 257.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 361.0 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 233.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 206.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 1> | 159.4 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 284.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 196.9 |
CdS (mp-672) | <1 0 1> | <1 -1 1> | 159.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 257.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 257.6 |
Te2W (mp-22693) | <0 1 1> | <1 -1 -1> | 171.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 272.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 328.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 222.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 284.2 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 170.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 220.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 291.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 328.1 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 222.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 361.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.00 | -0.03 | 0.03 |
-0.03 | 2.98 | 0.04 |
0.03 | 0.04 | 2.96 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.49 | -0.31 | -1.09 |
-0.31 | 9.16 | 0.75 |
-1.09 | 0.75 | 10.71 |
Polycrystalline dielectric constant
εpoly∞
2.98
|
Polycrystalline dielectric constant
εpoly
9.79
|
Refractive Index n1.73 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
In3Te3I (mp-616327) | 0.6496 | 0.000 | 3 |
Ag2PS3 (mp-558469) | 0.6548 | 0.002 | 3 |
Na4CO4 (mp-13274) | 0.6422 | 0.132 | 3 |
Hg3AsO4 (mp-4445) | 0.6483 | 0.006 | 3 |
Hg3PO4 (mp-29709) | 0.6113 | 0.010 | 3 |
Rb2Li2GeO4 (mp-8450) | 0.3519 | 0.000 | 4 |
Rb2Li2SiO4 (mp-8449) | 0.3087 | 0.000 | 4 |
Cs2Li2GeO4 (mp-8313) | 0.4388 | 0.000 | 4 |
Cs2Li2TiO4 (mp-8294) | 0.3647 | 0.000 | 4 |
Hg2PO3F (mp-561472) | 0.5893 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Li_sv Si O |
Final Energy/Atom-5.5914 eV |
Corrected Energy-106.2642 eV
-106.2642 eV = -100.6459 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)