Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.823 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.49 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.023 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P321 [150]
Hall
P 3 2"
Point Group
32
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.000 71.0
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.002 284.1
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.003 71.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.005 71.0
AlN (mp-661) <0 0 1> <0 0 1> 0.021 213.1
ZnO (mp-2133) <1 0 1> <1 0 0> 0.025 177.5
ZnO (mp-2133) <0 0 1> <1 1 0> 0.027 307.5
C (mp-48) <1 0 0> <1 1 0> 0.029 76.9
C (mp-48) <0 0 1> <1 1 0> 0.030 230.6
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.036 307.5
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.037 266.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.041 71.0
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.063 284.1
Au (mp-81) <1 1 1> <0 0 1> 0.068 213.1
Al (mp-134) <1 1 1> <1 1 0> 0.078 307.5
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.078 213.1
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.089 284.1
SiC (mp-11714) <0 0 1> <1 0 0> 0.099 221.9
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.102 153.8
SiC (mp-7631) <0 0 1> <1 0 0> 0.106 221.9
C (mp-66) <1 1 1> <0 0 1> 0.107 284.1
TbScO3 (mp-31119) <0 1 1> <1 0 0> 0.112 266.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.128 213.1
GaP (mp-2490) <1 1 1> <0 0 1> 0.137 213.1
Ni (mp-23) <1 0 0> <1 0 0> 0.144 221.9
GaN (mp-804) <1 0 0> <1 1 0> 0.152 153.8
Ag (mp-124) <1 1 1> <0 0 1> 0.154 213.1
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.174 355.1
GaN (mp-804) <0 0 1> <1 0 0> 0.182 355.1
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.188 355.1
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.199 307.5
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.199 266.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.203 284.1
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.211 221.9
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.216 133.2
Ni (mp-23) <1 1 0> <1 1 0> 0.219 153.8
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.220 153.8
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.220 142.1
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.225 310.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.227 310.7
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.233 307.5
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.254 230.6
ZnO (mp-2133) <1 1 1> <1 0 0> 0.277 355.1
MoSe2 (mp-1634) <1 0 1> <1 1 0> 0.286 153.8
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.294 221.9
TiO2 (mp-390) <1 1 1> <1 0 0> 0.306 266.3
SiC (mp-11714) <1 1 0> <1 0 0> 0.320 266.3
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.321 310.7
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.321 284.1
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.325 177.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
232 103 107 -2 0 0
103 232 107 2 0 0
107 107 183 0 0 0
-2 2 0 64 0 0
0 0 0 0 64 -2
0 0 0 0 -2 65
Compliance Tensor Sij (10-12Pa-1)
6.3 -1.5 -2.8 0.2 0 0
-1.5 6.3 -2.8 -0.2 0 0
-2.8 -2.8 8.8 0 0 0
0.2 -0.2 0 15.7 0 0
0 0 0 0 15.7 0.4
0 0 0 0 0.4 15.5
Shear Modulus GV
60 GPa
Bulk Modulus KV
142 GPa
Shear Modulus GR
59 GPa
Bulk Modulus KR
141 GPa
Shear Modulus GVRH
60 GPa
Bulk Modulus KVRH
142 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.32

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
-0.14335 0.14335 0.00000 -0.11828 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.11828 0.14335
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.23471 C/m2
Crystallographic Direction vmax
-1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.65 -0.00 0.00
-0.00 4.65 0.00
0.00 0.00 4.47
Dielectric Tensor εij (total)
12.50 -0.00 0.00
-0.00 12.50 0.00
0.00 0.00 13.28
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.59
Polycrystalline dielectric constant εpoly
(total)
12.76
Refractive Index n
2.14
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2GeF6 (mp-5368) 0.1614 0.000 3
Lu2TeO6 (mp-755515) 0.1275 0.000 3
Er2TeO6 (mp-755376) 0.1501 0.001 3
Tm2TeO6 (mp-772191) 0.1434 0.000 3
Sc2TeO6 (mp-557773) 0.1538 0.000 3
NaMnCrF6 (mp-618750) 0.2218 0.000 4
LiMnFeF6 (mp-555001) 0.1667 0.003 4
LiMnGaF6 (mp-558902) 0.1401 0.000 4
LiMnGaF6 (mp-704995) 0.1401 0.000 4
LiMnFeF6 (mp-648400) 0.1680 0.003 4
TiO2 (mp-775938) 0.3552 0.039 2
Rb2O (mp-755459) 0.3567 0.018 2
SiO2 (mp-32667) 0.3643 0.241 2
GeO2 (mp-10913) 0.3585 0.041 2
SnO2 (mp-12978) 0.3693 0.018 2
SrLaMnRuO6 (mp-39239) 0.6761 0.094 5
SrLaMnRuO6 (mp-690590) 0.6852 0.094 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d Te O
Final Energy/Atom
-5.6241 eV
Corrected Energy
-164.2166 eV
Uncorrected energy = -151.8506 eV Composition-based energy adjustment (-0.687 eV/atom x 18.0 atoms) = -12.3660 eV Corrected energy = -164.2166 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 60260
Submitted by
User remarks:
  • Diindium tellurium hexaoxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)