Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.057 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2Zn2O7 + ZnO |
Band Gap2.543 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 246.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 174.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 264.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 144.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 276.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 276.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 261.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 245.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 261.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 163.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 261.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 245.0 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 264.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 174.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 245.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 261.8 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 276.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 245.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 246.1 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 245.0 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 254.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 245.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 245.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 261.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 245.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 88.1 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 264.4 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 144.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 144.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 276.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 163.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 245.0 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 264.4 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 144.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 245.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 245.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 245.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 245.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 163.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 245.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 245.0 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 245.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 245.0 |
Au (mp-81) | <1 1 0> | <0 0 1> | 245.0 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 276.1 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 245.0 |
C (mp-48) | <0 0 1> | <1 0 -1> | 264.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 245.0 |
ZrO2 (mp-2858) | <1 0 -1> | <1 1 0> | 253.6 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 276.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(Si2O7)2 (mp-767345) | 0.5801 | 0.100 | 3 |
Cu4As2O9 (mp-21770) | 0.4881 | 0.022 | 3 |
Zn4As2O9 (mp-555797) | 0.3671 | 0.008 | 3 |
Cr4(PO4)3 (mp-540460) | 0.5999 | 0.324 | 3 |
Cr4(PO4)3 (mp-774538) | 0.5944 | 0.324 | 3 |
LiCuPO4 (mp-758170) | 0.6009 | 0.075 | 4 |
LiMn2(PO4)2 (mp-767083) | 0.5608 | 0.065 | 4 |
Li2Co(Si2O5)2 (mp-770682) | 0.6042 | 0.114 | 4 |
Li3Fe3(PO4)4 (mp-31797) | 0.5740 | 0.049 | 4 |
LiFeSiO4 (mp-762638) | 0.5804 | 0.097 | 4 |
LiFe3SiPO8 (mp-743761) | 0.7198 | 0.221 | 5 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.6743 | 0.004 | 5 |
Mg5Al4Fe(SiO4)6 (mp-743769) | 0.7261 | 0.280 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv Zn O |
Final Energy/Atom-5.9270 eV |
Corrected Energy-394.3583 eV
-394.3583 eV = -355.6198 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)