Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.868 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.171 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 175.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 175.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 219.8 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 162.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 307.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 272.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 296.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 99.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 68.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 243.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 197.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 351.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 351.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 266.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 197.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 307.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 162.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 111.8 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 197.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 68.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 243.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 131.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 162.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 197.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 197.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 351.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 68.1 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 162.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 197.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 219.8 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 272.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 263.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 68.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 219.8 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 243.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 307.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 307.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 131.9 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 266.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 131.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 307.7 |
BN (mp-984) | <1 1 0> | <1 0 1> | 99.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 197.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 131.9 |
Al (mp-134) | <1 1 0> | <0 1 1> | 162.1 |
Al (mp-134) | <1 1 1> | <1 0 1> | 197.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 99.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 131.9 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 219.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ReO5 (mp-505390) | 0.1771 | 0.000 | 3 |
Sr2WO5 (mp-772676) | 0.3184 | 0.005 | 3 |
Cs2DyCl5 (mp-540695) | 0.2249 | 0.000 | 3 |
Rb2FeF5 (mp-555378) | 0.3776 | 0.000 | 3 |
K2FeF5 (mp-565539) | 0.3242 | 0.000 | 3 |
ReSbOF10 (mp-554432) | 0.6103 | 0.000 | 4 |
K2TiOF4 (mp-556623) | 0.7500 | 0.000 | 4 |
K2VO2F3 (mp-18832) | 0.6791 | 0.000 | 4 |
K2RuNCl5O (mp-541361) | 0.7040 | 0.000 | 5 |
K2OsCBr5O (mp-556047) | 0.7390 | 0.000 | 5 |
KWNClF5 (mp-566462) | 0.7084 | 0.106 | 5 |
K2RuNCl5O (mp-560966) | 0.6858 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Ba_sv W_pv O |
Final Energy/Atom-7.0776 eV |
Corrected Energy-257.9749 eV
Uncorrected energy = -226.4829 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-4.438 eV/atom x 4.0 atoms) = -17.7520 eV
Corrected energy = -257.9749 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)