material

Si2Pd9

ID:

mp-505071

DOI:

10.17188/1262227


Tags: Palladium silicide (9/2)

Material Details

Final Magnetic Moment
0.013 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.455 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.19 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <1 0 1> <1 1 0> 0.002 113.5
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.034 263.1
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.042 263.1
ZnO (mp-2133) <0 0 1> <0 1 1> 0.054 299.5
CdS (mp-672) <0 0 1> <0 1 1> 0.055 199.7
C (mp-66) <1 1 1> <0 1 1> 0.055 199.7
CaCO3 (mp-3953) <0 0 1> <0 1 1> 0.059 199.7
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.060 138.3
Ni (mp-23) <1 1 1> <0 1 1> 0.060 299.5
ZnTe (mp-2176) <1 1 1> <0 1 1> 0.065 199.7
NdGaO3 (mp-3196) <1 0 1> <0 1 0> 0.072 216.0
CdSe (mp-2691) <1 1 1> <0 1 1> 0.073 199.7
InAs (mp-20305) <1 1 1> <0 1 1> 0.073 199.7
BN (mp-984) <1 0 0> <0 1 0> 0.080 288.0
GaSb (mp-1156) <1 1 1> <0 1 1> 0.093 199.7
GaN (mp-804) <1 0 1> <1 1 0> 0.102 113.5
MoSe2 (mp-1634) <0 0 1> <0 1 1> 0.114 199.7
WSe2 (mp-1821) <0 0 1> <0 1 1> 0.115 199.7
Al (mp-134) <1 1 1> <0 1 1> 0.117 199.7
Bi2Se3 (mp-541837) <0 0 1> <0 1 1> 0.117 199.7
PbSe (mp-2201) <1 1 1> <0 1 1> 0.127 199.7
SrTiO3 (mp-4651) <1 0 1> <0 1 0> 0.176 216.0
KTaO3 (mp-3614) <1 1 1> <0 1 1> 0.187 199.7
LiF (mp-1138) <1 1 1> <0 1 1> 0.192 199.7
KCl (mp-23193) <1 1 0> <1 0 0> 0.192 175.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 1 1> 0.193 199.7
YAlO3 (mp-3792) <1 0 0> <0 1 1> 0.195 199.7
LiNbO3 (mp-3731) <1 1 1> <1 0 0> 0.199 263.1
C (mp-48) <0 0 1> <1 0 0> 0.231 263.1
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.234 276.6
Mg (mp-153) <1 1 1> <0 1 1> 0.236 299.5
SiO2 (mp-6930) <0 0 1> <0 1 1> 0.257 199.7
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.259 87.7
BN (mp-984) <0 0 1> <1 0 1> 0.264 223.4
LaF3 (mp-905) <1 0 0> <0 1 0> 0.265 216.0
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.267 276.6
GaP (mp-2490) <1 0 0> <0 1 1> 0.293 299.5
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.294 276.6
Cu (mp-30) <1 1 0> <0 0 1> 0.315 276.6
SiC (mp-7631) <1 0 0> <0 0 1> 0.325 138.3
SiC (mp-11714) <1 0 0> <0 0 1> 0.329 276.6
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.360 207.4
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.363 207.4
C (mp-48) <1 0 0> <0 1 0> 0.369 288.0
Si (mp-149) <1 0 0> <0 0 1> 0.372 207.4
AlN (mp-661) <1 1 0> <0 1 1> 0.373 299.5
AlN (mp-661) <1 0 0> <0 1 0> 0.378 144.0
CaF2 (mp-2741) <1 0 0> <0 1 1> 0.380 299.5
BN (mp-984) <1 1 0> <0 1 1> 0.397 99.8
TeO2 (mp-2125) <0 1 1> <0 1 1> 0.415 299.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
248 126 119 0 0 0
126 240 132 0 0 0
119 132 230 0 0 0
0 0 0 38 0 0
0 0 0 0 19 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
6 -2.1 -1.9 0 0 0
-2.1 6.8 -2.8 0 0 0
-1.9 -2.8 6.9 0 0 0
0 0 0 26.5 0 0
0 0 0 0 52.3 0
0 0 0 0 0 31.7
Shear Modulus GV
40 GPa
Bulk Modulus KV
163 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
163 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
163 GPa
Elastic Anisotropy
0.91
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Y5(In2Pd)2 (mp-980936) 0.7482 0.000 3
Lu5(In2Ni)2 (mp-646321) 0.7407 0.000 3
Dy5(In2Ni)2 (mp-607124) 0.7335 0.000 3
Ni5As2 (mp-941) 0.6554 0.000 2
Mg6Si5 (mp-1073877) 0.6820 0.249 2
Mg2Si (mp-1074772) 0.6805 0.221 2
Mg2Si (mp-1074770) 0.6783 0.241 2
Mg7Si4 (mp-1074855) 0.6658 0.208 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Pd
Final Energy/Atom
-5.6764 eV
Corrected Energy
-249.7633 eV
Uncorrected energy = -249.7633 eV Corrected energy = -249.7633 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 67451
  • 648856
Submitted by
User remarks:
  • Palladium silicide (9/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)