Final Magnetic Moment0.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.899 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMgV4Cu3O14 + Mg2V2O7 + K3V5O14 + CuO |
Band Gap0.005 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 208.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 233.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 152.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 254.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 200.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 233.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 272.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 133.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 266.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 272.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 311.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 155.7 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 233.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 272.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 152.9 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 155.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 203.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 305.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 254.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 181.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 200.1 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 233.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 272.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 272.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 66.7 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 155.7 |
BN (mp-984) | <1 1 1> | <1 1 -1> | 239.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 51.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 200.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 -1> | 233.6 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 254.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 266.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 203.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 181.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 203.8 |
Al (mp-134) | <1 1 1> | <1 1 1> | 255.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 51.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 272.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 254.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 51.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 254.8 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 203.8 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 203.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 66.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 77.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 272.9 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 254.8 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 101.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 254.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: K_sv Mg_pv V_pv Cu_pv O |
Final Energy/Atom-6.2854 eV |
Corrected Energy-304.6202 eV
Uncorrected energy = -276.5582 eV
Composition-based energy adjustment (-0.687 eV/atom x 26.0 atoms) = -17.8620 eV
Composition-based energy adjustment (-1.700 eV/atom x 6.0 atoms) = -10.2000 eV
Corrected energy = -304.6202 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)