Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.365 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 362.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 286.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 114.4 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 291.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 190.7 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 109.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 324.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 255.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 95.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 133.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 182.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 133.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 114.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 323.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 152.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 362.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 133.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 328.0 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 291.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 185.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 148.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 95.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 109.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 133.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 323.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 190.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 109.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 286.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 209.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 266.9 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 292.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 273.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 57.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 255.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 273.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 133.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 133.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 95.3 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 198.1 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 218.7 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 145.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 133.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 95.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 57.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 95.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 114.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 156.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 259.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 291.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er2Mo2C3 (mp-3776) | 0.0411 | 0.000 | 3 |
Tm2Mo2C3 (mp-1025369) | 0.0921 | 0.000 | 3 |
Dy2Mo2C3 (mp-1025363) | 0.0405 | 0.000 | 3 |
Tb2Mo2C3 (mp-1025326) | 0.1024 | 0.000 | 3 |
Gd2Mo2C3 (mp-12039) | 0.1485 | 0.000 | 3 |
Li3Ti2Cu3O10 (mp-849652) | 0.5738 | 0.088 | 4 |
Li5Mn5CoO12 (mp-765276) | 0.5876 | 0.077 | 4 |
Li2V(OF)2 (mp-764218) | 0.5860 | 0.088 | 4 |
Li3Ti2Mn3O10 (mp-762872) | 0.5303 | 0.044 | 4 |
Li3Fe3(SnO5)2 (mp-762819) | 0.5747 | 0.072 | 4 |
Sr4N3 (mp-685023) | 0.6706 | 0.191 | 2 |
Cr3N4 (mp-1014365) | 0.6620 | 0.191 | 2 |
Fe3O4 (mp-705416) | 0.7157 | 0.143 | 2 |
Fe3O4 (mp-715614) | 0.6743 | 0.466 | 2 |
Cr3O4 (mp-772696) | 0.7017 | 0.082 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Mo_pv C |
Final Energy/Atom-8.7274 eV |
Corrected Energy-61.0916 eV
-61.0916 eV = -61.0916 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)