Final Magnetic Moment3.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.556 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn(SeO3)2 + Mn2O3 + MnSe2O5 |
Band Gap0.013 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 1 -1> | 169.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 270.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 289.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 270.5 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 193.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 67.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 202.8 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 96.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 202.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 270.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 289.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 202.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 289.8 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 289.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 67.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 135.2 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 193.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 289.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 193.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 270.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 202.8 |
C (mp-66) | <1 1 0> | <1 0 -1> | 289.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 270.5 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 270.5 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 270.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 193.2 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 135.2 |
InSb (mp-20012) | <1 1 0> | <1 0 -1> | 193.2 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 270.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 289.8 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 270.5 |
Si (mp-149) | <1 1 1> | <1 0 0> | 270.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 270.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 -1> | 193.2 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 202.8 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 135.2 |
NaCl (mp-22862) | <1 1 1> | <1 0 0> | 270.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 270.5 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 270.5 |
GaSb (mp-1156) | <1 0 0> | <1 0 -1> | 193.2 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 135.2 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 270.5 |
CaF2 (mp-2741) | <1 1 1> | <1 0 0> | 270.5 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 202.8 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 109.6 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 270.5 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 270.5 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 270.5 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 -1> | 289.8 |
ZnTe (mp-2176) | <1 0 0> | <1 0 -1> | 193.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NiSeO3 (mp-643029) | 0.5235 | 0.066 | 3 |
LiFeF4 (mp-777525) | 0.6430 | 0.371 | 3 |
Nb2Ge2O7 (mp-754857) | 0.6334 | 0.095 | 3 |
Fe2Se2O7 (mp-561440) | 0.4927 | 0.505 | 3 |
Fe4As5O13 (mp-505012) | 0.6078 | 0.090 | 3 |
MnNb2ZnO8 (mvc-15048) | 0.6849 | 0.087 | 4 |
Li2Mn3(SeO3)4 (mp-773608) | 0.6042 | 0.000 | 4 |
InHSeO4 (mp-560404) | 0.5844 | 0.000 | 4 |
LiFe(SeO3)2 (mp-566507) | 0.4809 | 0.124 | 4 |
YFe(WO4)2 (mvc-620) | 0.6289 | 0.054 | 4 |
Li2VH2OF5 (mp-861531) | 0.6490 | 0.185 | 5 |
Li2VH2OF5 (mp-770536) | 0.6652 | 0.054 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Se O |
Final Energy/Atom-6.2681 eV |
Corrected Energy-224.7088 eV
-224.7088 eV = -200.5779 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)