Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.844 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.362 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 1 0> | 233.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 233.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 210.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 93.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 93.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 281.5 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 93.8 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 233.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 310.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 315.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 125.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 233.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 93.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 233.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 263.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 281.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 93.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 281.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 315.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 233.1 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 210.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 263.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 93.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 210.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 233.1 |
Al (mp-134) | <1 1 1> | <0 1 1> | 281.5 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 187.7 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 281.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 263.0 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 125.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 187.7 |
BN (mp-984) | <1 0 1> | <0 1 1> | 281.5 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 93.8 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 77.7 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 77.7 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 263.0 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 263.0 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 263.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 263.0 |
Al (mp-134) | <1 1 0> | <0 1 1> | 93.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 210.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 281.5 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 210.4 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 210.4 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 93.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 93.8 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 233.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 263.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 125.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 263.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr2P2O7 (mp-5616) | 0.1384 | 0.000 | 3 |
BaAl2O6 (mp-867936) | 0.6425 | 0.442 | 3 |
K2Cr3O10 (mp-504618) | 0.6476 | 0.018 | 3 |
Rb2Cr2O7 (mp-19658) | 0.6574 | 0.001 | 3 |
Ba2P2O7 (mp-1019530) | 0.2550 | 0.000 | 3 |
NaCeP2O7 (mp-21520) | 0.3198 | 0.000 | 4 |
Rb3Al2(PO4)3 (mp-560459) | 0.6932 | 0.000 | 4 |
NaLaP2O7 (mp-560939) | 0.3054 | 0.000 | 4 |
Cs4Ba(PO3)6 (mp-560944) | 0.7021 | 0.000 | 4 |
KPSO2 (mp-1019891) | 0.7156 | 0.010 | 4 |
LaH4S2NO8 (mp-558126) | 0.5124 | 0.000 | 5 |
BaBePO4F (mp-754604) | 0.6864 | 0.000 | 5 |
K2Cr2AsHO10 (mp-744205) | 0.7304 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Pb_d P O |
Final Energy/Atom-7.0343 eV |
Corrected Energy-329.1717 eV
-329.1717 eV = -309.5075 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)