Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 153.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 126.8 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 153.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 126.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 173.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 150.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 150.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 260.2 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 260.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 253.6 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 260.2 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 260.2 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 260.2 |
C (mp-48) | <1 0 1> | <1 0 0> | 260.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 150.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.8 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 260.2 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 260.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 260.2 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 260.2 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 260.2 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 260.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2CaI6 (mp-753351) | 0.6425 | 0.090 | 3 |
Bi2OF4 (mp-753309) | 0.4564 | 0.012 | 3 |
Bi3O2F5 (mp-759405) | 0.5977 | 0.006 | 3 |
LaNdI4 (mp-569670) | 0.6324 | 0.105 | 3 |
Ba2SrI6 (mp-754408) | 0.5939 | 0.056 | 3 |
V3S (mp-7945) | 0.5688 | 0.003 | 2 |
MgSi (mp-1073857) | 0.5674 | 0.147 | 2 |
Mg4Si3 (mp-1074562) | 0.5401 | 0.187 | 2 |
Mg4Si3 (mp-1074591) | 0.5749 | 0.205 | 2 |
Mg2Si (mp-1074730) | 0.5808 | 0.144 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P Pd |
Final Energy/Atom-5.7235 eV |
Corrected Energy-114.4703 eV
-114.4703 eV = -114.4703 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)