material

CrCuO2

ID:

mp-505562

DOI:

10.17188/1262590


Tags: Copper(I) chromate(III) Copper(I) chromium(III) oxide

Material Details

Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.796 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
< 0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CrCuO2
Band Gap
1.870 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 82065 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbS (mp-21276) <1 1 1> <0 0 1> 0.000 249.5
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.001 152.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.001 201.2
PbSe (mp-2201) <1 1 1> <0 0 1> 0.001 201.2
C (mp-48) <1 1 1> <0 0 1> 0.005 169.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.005 201.2
NaCl (mp-22862) <1 1 1> <0 0 1> 0.009 56.3
LiF (mp-1138) <1 1 1> <0 0 1> 0.012 201.2
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.014 128.8
Mg (mp-153) <0 0 1> <0 0 1> 0.025 104.6
CdS (mp-672) <1 0 0> <0 0 1> 0.030 201.2
Mg (mp-153) <1 1 0> <0 0 1> 0.033 144.9
ZnO (mp-2133) <1 1 0> <1 1 0> 0.037 60.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.049 152.9
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.053 169.0
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.065 225.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.067 104.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.067 104.6
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.074 104.6
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.076 314.1
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.077 152.9
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.079 201.2
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.081 48.3
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.081 193.2
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.083 161.0
ZnO (mp-2133) <1 0 0> <1 1 0> 0.090 120.9
C (mp-66) <1 1 1> <0 0 1> 0.092 152.9
InAs (mp-20305) <1 1 1> <0 0 1> 0.093 201.2
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.096 354.1
LiNbO3 (mp-3731) <1 0 1> <0 0 1> 0.096 233.4
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.101 56.3
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.105 128.8
BN (mp-984) <1 0 0> <0 0 1> 0.109 152.9
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.112 174.5
Cu (mp-30) <1 0 0> <0 0 1> 0.112 144.9
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.115 181.4
InP (mp-20351) <1 1 1> <0 0 1> 0.115 249.5
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.117 161.0
Ge3(BiO3)4 (mp-23560) <1 1 0> <0 0 1> 0.118 161.0
KCl (mp-23193) <1 1 0> <0 0 1> 0.119 289.7
Te2W (mp-22693) <0 1 0> <0 0 1> 0.120 161.0
Al (mp-134) <1 1 0> <0 0 1> 0.124 161.0
Mg (mp-153) <1 1 1> <0 0 1> 0.128 209.3
MgO (mp-1265) <1 1 0> <0 0 1> 0.129 128.8
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.133 152.9
TiO2 (mp-390) <1 0 1> <1 1 0> 0.135 120.9
Si (mp-149) <1 1 1> <0 0 1> 0.141 152.9
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.145 144.9
GaAs (mp-2534) <1 1 1> <0 0 1> 0.146 56.3
InAs (mp-20305) <1 1 0> <0 0 1> 0.148 161.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
227 70 112 0 0 0
70 227 112 0 0 0
112 112 427 0 0 0
0 0 0 29 0 0
0 0 0 0 29 0
0 0 0 0 0 79
Compliance Tensor Sij (10-12Pa-1)
5.3 -1.1 -1.1 0 0 0
-1.1 5.3 -1.1 0 0 0
-1.1 -1.1 2.9 0 0 0
0 0 0 34.1 0 0
0 0 0 0 34.1 0
0 0 0 0 0 12.7
Shear Modulus GV
67 GPa
Bulk Modulus KV
163 GPa
Shear Modulus GR
48 GPa
Bulk Modulus KR
145 GPa
Shear Modulus GVRH
58 GPa
Bulk Modulus KVRH
154 GPa
Elastic Anisotropy
2.01
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TlAgO2 (mp-997010) 0.1075 0.000 3
CrCuO2 (mp-510625) 0.0947 0.000 3
CrCuO2 (mp-773929) 0.0111 0.000 3
CrCuO2 (mp-773729) 0.0048 0.000 3
CrCuO2 (mp-796545) 0.0957 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Cr: 3.7 eV
Pseudopotentials
VASP PAW: Cr_pv Cu_pv O
Final Energy/Atom
-6.8533 eV
Corrected Energy
-61.5720 eV
Uncorrected energy = -54.8260 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Composition-based energy adjustment (-1.999 eV/atom x 2.0 atoms) = -3.9980 eV Corrected energy = -61.5720 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 82065
  • 402289
Submitted by
User remarks:
  • Copper(I) chromate(III)