Final Magnetic Moment0.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.697 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH2O + CePO4 + H2 + P |
Band Gap0.064 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 226.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 226.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 226.1 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 231.8 |
AlN (mp-661) | <1 1 0> | <1 -1 1> | 270.0 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 133.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 169.5 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 100.5 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 332.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 169.5 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 0> | 231.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 324.5 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 203.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 324.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 309.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 324.5 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 201.1 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 1> | 270.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 296.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 0> | 309.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 -1> | 266.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 231.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 282.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 226.1 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 199.7 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 154.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 332.9 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 324.5 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 77.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 324.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 194.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 -1> | 133.1 |
Al (mp-134) | <1 1 0> | <1 0 1> | 296.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 98.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 266.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 226.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 339.1 |
MgO (mp-1265) | <1 0 0> | <1 -1 0> | 231.8 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 129.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 282.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 205.0 |
Mg (mp-153) | <1 0 0> | <1 -1 1> | 270.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 -1> | 266.3 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 -1> | 231.5 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 282.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 324.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 194.7 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 141.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 -1 1> | 270.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 -1 1> | 270.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaS3O10 (mp-1019581) | 0.7098 | 0.000 | 3 |
Nd2P3(HO2)5 (mp-707307) | 0.3909 | 0.014 | 4 |
PrP2(HO)7 (mp-734771) | 0.2775 | 0.020 | 4 |
Pr2P3(HO2)5 (mp-722780) | 0.3829 | 0.014 | 4 |
LaP3H8O7 (mp-697701) | 0.1486 | 0.040 | 4 |
LuH6(ClO5)3 (mp-757220) | 0.3744 | 0.000 | 4 |
SmH8S3N3O10 (mp-782002) | 0.4189 | 0.065 | 5 |
SmH10S3N3O11 (mp-781997) | 0.3700 | 0.065 | 5 |
ZrH6NOF5 (mp-707811) | 0.5012 | 0.000 | 5 |
UP3H10BrO8 (mp-740732) | 0.4343 | 0.043 | 5 |
UP3H10ClO8 (mp-730972) | 0.3442 | 0.055 | 5 |
K2H2C3S2O7F6 (mp-699253) | 0.4452 | 0.230 | 6 |
RbC2S2N(OF)4 (mp-559029) | 0.6342 | 0.250 | 6 |
H18PbC6S4N2O9 (mp-559034) | 0.5584 | 0.247 | 6 |
HoH16C2S2NO12 (mp-555297) | 0.7450 | 0.066 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce P H O |
Final Energy/Atom-5.7922 eV |