Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.267 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.404 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 -1> | 282.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 327.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 196.4 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 286.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 202.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 261.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 286.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 303.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 196.4 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 219.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 206.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 202.5 |
GaN (mp-804) | <1 1 1> | <1 -1 0> | 219.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 202.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 196.4 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 -1> | 282.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 261.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 185.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 253.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 154.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 292.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 278.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 271.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 151.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 206.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 286.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 232.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 286.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 154.8 |
Te2W (mp-22693) | <1 1 1> | <1 -1 0> | 219.1 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 95.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 253.2 |
YVO4 (mp-19133) | <1 0 0> | <0 1 -1> | 135.6 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 275.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 151.9 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 0> | 219.1 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 278.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 261.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 151.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 278.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 203.4 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 278.2 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 278.2 |
BN (mp-984) | <0 0 1> | <1 -1 0> | 219.1 |
BN (mp-984) | <1 0 1> | <0 1 0> | 261.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 -1 -1> | 282.3 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 137.6 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 232.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 261.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
As2Pb3O8 (mp-505368) | 0.6112 | 0.000 | 3 |
Bi2MoO6 (mp-557388) | 0.6650 | 0.004 | 3 |
V2Pb3O8 (mp-25726) | 0.6429 | 0.000 | 3 |
V2Pb3O8 (mp-25142) | 0.5909 | 0.003 | 3 |
Bi3(PO5)2 (mvc-15217) | 0.5852 | 0.074 | 3 |
BaBi6(PO5)4 (mp-554084) | 0.3162 | 0.000 | 4 |
Na2Th(PO4)2 (mp-582483) | 0.5643 | 0.000 | 4 |
SrV4(Bi3O10)2 (mp-565761) | 0.4584 | 0.000 | 4 |
SrBi6(PO5)4 (mp-561005) | 0.0697 | 0.000 | 4 |
CaBi6(PO5)4 (mvc-16369) | 0.2635 | 0.000 | 4 |
KBiS(ClO2)2 (mp-23645) | 0.7111 | 0.000 | 5 |
KSnSO4F (mp-557399) | 0.6532 | 0.000 | 5 |
K2Sb2S(O2F3)2 (mp-557470) | 0.6372 | 0.000 | 5 |
BaCaVP2O9 (mvc-16553) | 0.7182 | 0.003 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi P Pb_d O |
Final Energy/Atom-6.5771 eV |
Corrected Energy-217.9346 eV
-217.9346 eV = -203.8888 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)